Tensile Strength, Ultimate | 29.0 - 51.0 MPa | 4210 - 7400 psi | Average value: 39.7 MPa Grade Count:14 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m.. |
|||
Tensile Strength, Ultimate | 1.40 - 51.0 MPa @Temperature -20.0 - 49.0 °C |
203 - 7400 psi @Temperature -4.00 - 120 °F |
Average value: 19.8 MPa Grade Count:11 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate; Molded/Extruded". Each property range of values reported is minimum and maximum .. |
|||
Tensile Strength, Ultimate | 14.0 - 51.0 MPa | 2030 - 7400 psi | Average value: 38.4 MPa Grade Count:15 |
Overview of materials for PVC, Powder This property data is a summary of similar materials in the MatWeb database for the category "PVC, Powder". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Tensile Strength, Ultimate | 0.255 - 51.0 MPa | 37.0 - 7400 psi | Average value: 9.26 MPa Grade Count:573 |
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Elastomer, Melt-Processible Rubber". Each property range of values reported is minimum and.. |
|||
Tensile Strength, Ultimate | 0.150 - 51.0 MPa | 21.8 - 7400 psi | Average value: 27.7 MPa Grade Count:22 |
Overview of materials for Polystyrene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Tensile Strength, Ultimate | 23.0 - 51.0 MPa @Temperature 60.0 - 120 °C |
3340 - 7400 psi @Temperature 140 - 248 °F |
Average value: 38.1 MPa Grade Count:4 |
Overview of materials for Polycarbonate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri.. |