Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 35.0 - 250 MPa @Temperature 60.0 - 275 °C |
5080 - 36300 psi @Temperature 140 - 527 °F |
Average value: 134 MPa Grade Count:14 |
Overview of materials for Polyetheretherketone, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
Tensile Strength, Ultimate | 14.0 - 250 MPa @Temperature -40.0 - 250 °C |
2030 - 36300 psi @Temperature -40.0 - 482 °F |
Average value: 83.4 MPa Grade Count:3 |
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an.. |
|||
Tensile Strength, Ultimate | 14.0 - 250 MPa @Thickness 0.800 - 3.17 mm |
2030 - 36300 psi @Thickness 0.0315 - 0.125 in |
Average value: 83.4 MPa Grade Count:3 |
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an.. |
|||
Tensile Strength, Ultimate | 68.0 - 250 MPa | 9860 - 36300 psi | Average value: 143 MPa Grade Count:110 |
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Tensile Strength, Ultimate | 60.0 - 250 MPa | 8700 - 36300 psi | Average value: 131 MPa Grade Count:27 |
Overview of materials for Nylon 12, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Tensile Strength, Ultimate | 230 - 250 MPa | 33400 - 36300 psi | |
AMT AM-Lite® Die Casting Magnesium Alloy AM-lite is a high surface finish die casting alloy suitable for applications that currently utilize zinc, aluminum or magnesium (alloy AZ91D) die castings, or plastic injection moldings. AM-lite has.. |