Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 40.0 - 200 MPa @Temperature -40.0 - 140 °C |
5800 - 29000 psi @Temperature -40.0 - 284 °F |
Average value: 93.9 MPa Grade Count:1 |
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25.. |
|||
Tensile Strength, Ultimate | 40.0 - 200 MPa @Strain 0.500 - 5.00 % |
5800 - 29000 psi @Strain 0.500 - 5.00 % |
Average value: 93.9 MPa Grade Count:1 |
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25.. |
|||
Tensile Strength, Ultimate | 9.25 - 200 MPa | 1340 - 29000 psi | Average value: 101 MPa Grade Count:35 |
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are.. |
|||
Tensile Strength, Ultimate | 131 - 200 MPa | 19000 - 29000 psi | Average value: 170 MPa Grade Count:5 |
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled". Each property range of values reported i.. |
|||
Tensile Strength, Ultimate | 177 - 200 MPa | 25600 - 29000 psi | Average value: 187 MPa Grade Count:5 |
Overview of materials for Polyetherimide (PEI), 40% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 40% Glass Fiber". Specific grades with glass content between 35% and 44% are included. E.. |
|||
Tensile Strength, Ultimate | 100 - 200 MPa | 14500 - 29000 psi | Average value: 162 MPa Grade Count:12 |
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled". Specific grades with glass content between 15% an.. |
|||
Tensile Strength, Ultimate | 102 - 200 MPa | 14800 - 29000 psi | Average value: 148 MPa Grade Count:17 |
Overview of materials for Liquid Crystal Polymer (LCP), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Carbon Fiber Filled". Each property range of values reported is minimum an.. |
|||
Tensile Strength, Ultimate | 48.0 - 200 MPa @Temperature -40.0 - 150 °C |
6960 - 29000 psi @Temperature -40.0 - 302 °F |
Average value: 86.6 MPa Grade Count:1 |
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max.. |
|||
Tensile Strength, Ultimate | 36.5 - 200 MPa | 5300 - 29000 psi | Average value: 147 MPa Grade Count:17 |
Overview of materials for Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler". Specific grades with glass content between 45%.. |
|||
Tensile Strength, Ultimate | 50.0 - 200 MPa | 7250 - 29000 psi | Average value: 132 MPa Grade Count:127 |
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma.. |
|||
Tensile Strength, Ultimate | 44.8 - 200 MPa | 6500 - 29000 psi | Average value: 131 MPa Grade Count:141 |
Overview of materials for Nylon 612, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of .. |
|||
Tensile Strength, Ultimate | 100 - 200 MPa | 14500 - 29000 psi | Average value: 150 MPa Grade Count:17 |
Overview of materials for Nylon 46, Flame Retarded + Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Flame Retarded + Glass Fiber Reinforced". Each property range of values reported is minimum an.. |
|||
Tensile Strength, Ultimate | 22.4 - 200 MPa @Temperature -40.0 - 150 °C |
3250 - 29000 psi @Temperature -40.0 - 302 °F |
Average value: 87.1 MPa Grade Count:1 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |
|||
Tensile Strength, Ultimate | 22.4 - 200 MPa @Strain 0.140 - 4.69 % |
3250 - 29000 psi @Strain 0.140 - 4.69 % |
Average value: 87.1 MPa Grade Count:1 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |
|||
Tensile Strength, Ultimate | 22.0 - 200 MPa | 3190 - 29000 psi | Average value: 62.0 MPa Grade Count:104 |
Overview of materials for Nylon 6, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri.. |