Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 600 MPa | 87000 psi | Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4301 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Tensile Strength, Ultimate | 600 MPa | 87000 psi | Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4845 High Temperature Austenitic Stainless Steel Standardized high-temperature steel for use at temperatures up to 1100°C in dry air. Prone to embrittlement after exposure between 600-900°C. Applications: Heat and creep resistance. For use o.. |
|||
Tensile Strength, Ultimate | 600 MPa | 87000 psi | |
PSM Industries Pacific Sintered Metals Infiltrated High Carbon Steel FX-232-T Powdered Metal Good strength, shock resistance and hardenability, Moderate tolerance control Equivalent MPIF Specification: FX-1008-50Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Tensile Strength, Ultimate | 600 - 720 MPa | 87000 - 104000 psi | Typical |
Industeel SUPERELSO® 500 Quenched and Tempered High Strength Steel for Pressure Equipment Description: Superelso® 500 (SE 500) is a 500MPa (72ksi) yield strength quenched and tempered steel adapted for pressure equipment. SE 500 is manufactured via the electric furnace with dephosphor.. |
|||
Tensile Strength, Ultimate | 600 MPa @Temperature 760 °C |
87000 psi @Temperature 1400 °F |
|
Haynes 25 alloy, cold worked sheet, 10% cold reduction Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Tensile Strength, Ultimate | 600 MPa @Temperature 760 °C |
87000 psi @Temperature 1400 °F |
|
Haynes 625 alloy, cold rolled and 1050°C mill-annealed sheet Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Tensile Strength, Ultimate | 600 MPa | 87000 psi | Annealed prior to test |
Special Metals INCOLOY® Alloy 330 A nickel-iron-chromium alloy with an addition of silicon for enhanced oxidation resistance. It has good strength at high temperatures and excellent resistance to carburizing and oxidizing atmospher.. |
|||
Tensile Strength, Ultimate | 600 MPa | 87000 psi | Annealed |
Special Metals INCOLOY® Alloy 800 A nickel-iron-chromium alloy with good strength and excellent resistance to oxidation and carburization in high-temperature atmospheres. It also resists corrosion by many aqueous environments. The.. |
|||
Tensile Strength, Ultimate | 600 - 700 MPa | 87000 - 102000 psi | |
SSAB Tunnplat Docol® 600DP High-strength Steel High-strength SteelComments: Docol DP - Cold Rolled Steel - Extra high-strength steel (EHS). Property values are for cold-rolled steel; thicknesses 0.5 - 1.6 mm. Iron content is approximate - exact.. |
|||
Tensile Strength, Ultimate | 600 MPa | 87000 psi | |
SSAB Tunnplat Domex® 034 BOR Rolled Boron Steel Domex® is the brand name of hot rolled products from SSAB Tunnplat. Compared to conventional quenched and tempered steels, boron steel have several benefits including better formability. Boron .. |
|||
Tensile Strength, Ultimate | 600 - 760 MPa | 87000 - 110000 psi | |
SSAB Tunnplat Domex® 550MC HSLA Steel HSLA SteelCharacteristics: Domex® MC grade steels conform to the provisions of EN 10149-2 standard and often have better properties.Property data is for hot-rolled steel..Domex® is the brand n.. |
|||
Tensile Strength, Ultimate | 600 MPa | 87000 psi | |
Universal Wire Works 308 Stainless Steel Electrode Universal 308 coated electrodes are used for welding unstabilized 18-8 stainless steels such as types 301, 302, 302B, 303, 308Se 304, 305, and 308. Universal 308 electrodes provide corrosion resista.. |
|||
Tensile Strength, Ultimate | 600 MPa | 87000 psi | |
Universal Wire Works 309 Stainless Steel Electrode Universal 309 electrodes are used for the welding of heat resisting type 309 stainless steel. Deposits retain strength and oxidation resistance up to 2000 degrees F. Typical applications include fur.. |
|||
Tensile Strength, Ultimate | 600 MPa | 87000 psi | Typical |
TIMET TIMETAL® Code 12 Titanium Alloy (ASTM Grade 12) Features: Highly weldable, near-alpha alloy, exhibiting improved strength and temperature capability over CP combined with superior crevice corrosion resistance and excellent resistance under oxidiz.. |
|||
Tensile Strength, Ultimate | 600 - 696 MPa | 87000 - 101000 psi | |
Eagle Brass 64725 MAX251C, Hard Max 251c has an excellent balance in hardness, formability and conductivity. Typical uses include lead frames, circuit breakers, connectors, electrical springs, contact terminals, and fuse clips.In.. |
|||
Tensile Strength, Ultimate | >= 600 MPa | >= 87000 psi | |
CLAL-MSX NICLAL 3444 H14 4/4 Hard Copper Alloy, diameter < 8 Copper Alloy, Free Cutting Bronze Main Characteristics: Excellent machineabilityHigh mechanical propertiesSelf lubricating alloyTypical Applications:Parts for connectorsFriction partsBearings-Pinions-Lock pinsInformation provided b.. |
|||
Tensile Strength, Ultimate | >= 600 MPa | >= 87000 psi | Rod |
CLAL-MSX ARCAP Anticorrosion AP1 H15 Spring, Drawn Copper Alloy Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin.. |
|||
Tensile Strength, Ultimate | 600 - 750 MPa | 87000 - 109000 psi | |
CLAL-MSX ARCAP Anticorrosion AP1D H14 4/4 hard, Drawn Copper Alloy, Wire and rod, 2.5< diameter< 5 High Corrosion Resistance: ARCAP alloys are very corrosion resistant to the majority of chemical and physical environments. CLAL can provide data for the corrosion resistance of ARCAP alloys. In par.. |
|||
Tensile Strength, Ultimate | 600 - 680 MPa | 87000 - 98600 psi | |
CLAL-MSX DECLAFOR® 1015 TD3 Wire quenched/Cold Rolled Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Tensile Strength, Ultimate | 600 MPa | 87000 psi | Typical |
ATI Allegheny Ludlum Stainless Steel Ohmaloy® 40 Resistance Alloy Ohmaloy 40 alloy is a moderately magnetic, ductile stainless steel having extremely high electrical resistivity. In addition to imparting high electrical resistivity, the aluminum content in these .. |
|||
Tensile Strength, Ultimate | 600 - 700 MPa | 87000 - 102000 psi | |
ArcelorMittal Dual Phase 600 Very high strength steel, Cold Rolled Steel Available in the following: HCT780X (uncoated), HCT780X+ZE (electrogalvanized) and HCT780X+Z/ZF (Extragal®/Galvannealed)Description: Dual Phase steels offer an outstanding combination of strength a.. |
|||
Tensile Strength, Ultimate | 600 MPa | 87000 psi | Typical; after 1800°F Anneal |
ATI Allegheny Ludlum Type 332 Stainless Steel, UNS N08800 Type 332 is a nickel and chromium austenitic stainless steel designed to resist oxidation and carburization at elevated temperatures. The nickel content, 32%, makes the alloy highly resistant both .. |
|||
Tensile Strength, Ultimate | 600 MPa @Temperature 204 °C |
87000 psi @Temperature 399 °F |
|
ATI Allegheny Ludlum AL 2003™ Duplex Stainless Steel Characteristics: superior stress corrosion cracking resistance to Types 316 and 317, yield strength double that of conventional austenitic stainless steel, good corrosion resistance, good chloride s.. |
|||
Tensile Strength, Ultimate | 600 MPa | 87000 psi | Typical; Annealed at 1800°F (982°C) |
ATI Allegheny Ludlum AL 800™ Nickel-Base Alloy, UNS N08800 AL 800 alloy is nickel-iron-chromium alloys designed to resist oxidation and carburization at elevated temperatures. The nickel content makes the alloy highly resistant both to chloride stress-corr.. |
|||
Tensile Strength, Ultimate | 600 - 700 MPa | 87000 - 102000 psi | |
ArcelorMittal Complex Phase Steel 600 Very high strength steel, Cold Rolled Steel Available in the following: uncoated (HCT600C) and electrogalvanized (HCT600C+ZE)Description: The Complex Phase family of steels supplements ArcelorMittal's VHSS (very high strength steel) product r.. |
|||
Tensile Strength, Ultimate | 600 MPa | 87000 psi | Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4948 High Temperature Austenitic Stainless Steel Creep-resistant variant of 1.4301, with a standardized minimum carbon content for service at temperatures of up to 800°C in dry air.Applications: Heat and creep resistance. For use over 550°C for.. |
|||
Tensile Strength, Ultimate | 600 MPa | 87000 psi | Typical |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420HC Allegheny Ludlum Type 420HC is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainl.. |
|||
Tensile Strength, Ultimate | 600 MPa | 87000 psi | Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 904L High Performance Austenitic Stainless Steel Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar.. |
|||
Tensile Strength, Ultimate | 600 MPa @Temperature 538 °C |
87000 psi @Temperature 1000 °F |
|
Haynes Hastelloy® C-22® alloy, all-weld metal, GTAW HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |