Material Notes:
Description: Superelso® 500 (SE 500) is a 500MPa (72ksi) yield strength quenched and tempered steel adapted for pressure equipment. SE 500 is manufactured via the electric furnace with dephosphorisation, ladle refining and vacuum degassing to provide a reproducible, clean and homogeneous steel. The chemistry of SE 500 has been carefully adapted to combine high strength and excellent weldability. This steel also displays excellent toughness, with transition temperatures typically below -50°C/-58°F. This steel is particularly suitable for pressure equipment in the offshore oil and gas industry, where its high strength allows significant weight and cost reductions. It can be supplied with stainless steel or alloy cladding where necessary.Mechanical properties for 150 mm plates or thinner.Information provided by manufacturer.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 600 - 720 MPa
87000 - 104000 psi
Typical
Tensile Strength, Yield >= 500 MPa

@Strain 0.200 %
>= 72500 psi

@Strain 0.200 %
Elongation at Break 18 %
18 %
Typical
Charpy Impact >= 50.0 J

@Temperature >=-50.0 °C
>= 36.9 ft-lb

@Temperature >=-58.0 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.13 %
<= 0.13 %
Iron, Fe 96.356 - 100 %
96.356 - 100 %
As remainder
Manganese, Mn <= 1.6 %
<= 1.6 %
Molybdenum, Mo <= 0.50 %
<= 0.50 %
Nickel, Ni <= 1.0 %
<= 1.0 %
Phosphorous, P <= 0.010 %
<= 0.010 %
Silicon, Si <= 0.40 %
<= 0.40 %
Sulfur, S <= 0.0040 %
<= 0.0040 %