Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 51.7 MPa | 7500 psi | |
Mykroy/Mycalex MM 561 Molding Grade Glass-bonded Mica Composite Synthetic mica filler. Does not burn. Good radiation resistance (3 x 10^10 Rads-Cobalt). ROHS CompliantThis ceramoplastic material is a versatile and efficient insulating material designed to meet.. |
|||
Tensile Strength, Ultimate | 51.7 MPa | 7500 psi | ASTM D638 |
Nylene® Vexel™ B50U , High Flow, Un-reinforced PBT Description: Vexel™ B50U is a high flow, un-reinforced PBT. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporatio.. |
|||
Tensile Strength, Ultimate | 51.7 - 241 MPa | 7500 - 35000 psi | Average value: 94.5 MPa Grade Count:21 |
Overview of materials for Polyphthalamide (PPA), Aramid Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Aramid Fiber". Each property range of values reported is minimum and maximum values of .. |
|||
Tensile Strength, Ultimate | 51.7 - 2070 MPa | 7500 - 300000 psi | Average value: 207 MPa Grade Count:186 |
Overview of materials for Polyetheretherketone, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
Tensile Strength, Ultimate | 51.7 MPa | 7500 psi | ASTM Data |
Americas Styrenics Styron® 613 Polystyrene
(discontinued **) STYRON® 613 high heat, high strength general purpose polystyrene is typically used in applications requiring a clear, tough part such as office products and magnetic media enclosures. It offers goo.. |
|||
Tensile Strength, Ultimate | 51.7 MPa | 7500 psi | |
Indium Corp. Indalloy® 106 (Sn63) Sn-Pb Solder Alloy Standard eutectic tin-lead solder with wide application. Not recommended against silver and/or gold.Information provided by the manufacturer, Indium Corporation. |
|||
Tensile Strength, Ultimate | 51.7 MPa @Temperature 149 °C |
7500 psi @Temperature 300 °F |
|
Greene Tweed Arlon® 1000 Polyketone Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie.. |
|||
Tensile Strength, Ultimate | 51.7 MPa | 7500 psi | ASTM D638-95 |
Multibase Multi-ABS 7522 R , 22% Filler Content Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 51.7 MPa | 7500 psi | ASTM D638 |
Saint-Gobain Meldin® 7022 Isostatically Molded Graphite Filled Polyimide Finished parts and basic shapes made from 40% by weight graphite filled polyimide material for applications requiring a low coefficient of thermal expansion, self lubricating properties, and good di.. |
|||
Tensile Strength, Ultimate | 51.7 MPa | 7500 psi | |
Williams Advanced Alloys WS183 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Tensile Strength, Ultimate | 51.7 MPa | 7500 psi | ASTM D412 |
Lubrizol Estane® ETE 70DT3 Thermoplastic Polyurethane, Easy-to-Extrude Type: Estane® ETE 70DT3 is an aromatic polyether-based thermoplastic polyurethane (TPU).Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, hig.. |
|||
Tensile Strength, Ultimate | 51.7 MPa | 7500 psi | Crosswise; ASTM D638 |
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 1/8" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Tensile Strength, Ultimate | 51.7 MPa | 7500 psi | Crosswise; ASTM D638 |
Bedford Plastics Glass Reinforced Vinylester Flat Sheet, 1/8" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Tensile Strength, Ultimate | 51.7 MPa | 7500 psi | Crosswise; ASTM D638 |
Bedford Plastics Glass Reinforced Polyester Flat Sheet 1/8" Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |
|||
Tensile Strength, Ultimate | 51.7 - 70.0 MPa | 7500 - 10200 psi | Average value: 61.7 MPa Grade Count:6 |
Overview of materials for PC/ABS + Stainless Steel This property data is a summary of similar materials in the MatWeb database for the category "PC/ABS + Stainless Steel". Each property range of values reported is minimum and maximum values of appro.. |
|||
Tensile Strength, Ultimate | 51.7 - 124 MPa | 7500 - 18000 psi | Average value: 81.9 MPa Grade Count:11 |
Overview of materials for Acrylic/Polycarbonate Alloy, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Glass Fiber Filler". Each property range of values reported is minimum and .. |
|||
Tensile Strength, Ultimate | 51.7 MPa | 7500 psi | TM R050-36 |
Resinlab® EP1026 Clear Epoxy Adhesive Resinlab™ EP1026 Clear is a two part unfilled epoxy adhesive designed for high speed bonding of metals, ceramics, and most plastics. It cures to a tough semi-rigid material, and is free flowing in .. |
|||
Tensile Strength, Ultimate | 51.7 MPa | 7500 psi | TM R050-36 |
Resinlab® EP11HT Gray Filled Epoxy Adhesive Resinlab™ EP11HT Gray is a two part filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-rigid material. It has good wetting to most surfa.. |
|||
Tensile Strength, Ultimate | 51.7 MPa | 7500 psi | TM R050-36 |
Resinlab® EP965SC-7 Black Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP965SC-7 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wett.. |
|||
Tensile Strength, Ultimate | 51.7 MPa | 7500 psi | TM R050-36 |
Resinlab® EP965SC-7 Clear Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP965SC-7 Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wett.. |
|||
Tensile Strength, Ultimate | 51.7 MPa | 7500 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® UR-30GF/000 Thermoplastic Elastomer - TPU, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 51.7 MPa | 7500 psi | Film; ASTM D412 |
AdvanSource Biomaterials ChronoFlex® AR Biodurable Medical Grade Polyurethane AdvanSource Biomaterials Corporation manufactures and markets this solution-grade, segmented, aromatic, polycarbonate-based polyurethane designed for use in solvent casting and dipping applications... |
|||
Tensile Strength, Ultimate | 51.7 MPa | 7500 psi | TM R050-36 |
Resinlab® EP1026 Black Epoxy Adhesive Resinlab™ EP1026 Black is a two part unfilled epoxy adhesive designed for high speed bonding of metals, ceramics, and most plastics. It cures to a tough semi-rigid material, and is free flowing in .. |
|||
Tensile Strength, Ultimate | 51.7 - 72.4 MPa | 7500 - 10500 psi | ASTM D638 |
Premix Premi-Glas® 1200H-24 Polyester SMC
(discontinued **) Premi-Glas® 1200H-24 is a 24% fiberglass reinforced, thermoset, Sheet Molding Compound designed for applications where arc resistance and dielectric strength are required and UL 94 HB flame recogni.. |