Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 725 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 5.00 MPa
725 psi
ASTM D638-95
Multibase Multi-Flex® TPO A-7507
TPO compound suitable for carpet backing seals.Data provided by Multibase.
Tensile Strength, Ultimate 5.00 - 90.0 MPa

@Temperature -40.0 - 160 °C
725 - 13100 psi

@Temperature -40.0 - 320 °F
Average value: 38.8 MPa Grade Count:1
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim..
Tensile Strength, Ultimate 5.00 - 90.0 MPa

@Strain 2.00 - 10.0 %
725 - 13100 psi

@Strain 2.00 - 10.0 %
Average value: 38.8 MPa Grade Count:1
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim..
Tensile Strength, Ultimate 5.00 MPa
725 psi
ASTM D638
Total Finaprene® 411x Styrene-Butadiene TPE Copolymer Compounded to 57 Shore A  (discontinued **)
Styrene-Butadiene CopolymerDescription: Finaprene® 411x is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its high molecular weight, Finaprene® 411x provides e..
Tensile Strength, Ultimate 5.00 - 117 MPa
725 - 17000 psi
Average value: 53.3 MPa Grade Count:181
Overview of materials for Acetal Copolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of..
Tensile Strength, Ultimate 5.00 - 50.0 MPa

@Temperature 60.0 - 120 °C
725 - 7250 psi

@Temperature 140 - 248 °F
Average value: 26.0 MPa Grade Count:1
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi..
Tensile Strength, Ultimate 5.00 - 163 MPa

@Strain 0.270 - 12.0 %
725 - 23600 psi

@Strain 0.270 - 12.0 %
Average value: 66.6 MPa Grade Count:2
Overview of materials for Nylon 66, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..
Tensile Strength, Ultimate 5.00 - 163 MPa

@Temperature -40.0 - 230 °C
725 - 23600 psi

@Temperature -40.0 - 446 °F
Average value: 66.6 MPa Grade Count:2
Overview of materials for Nylon 66, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..
Tensile Strength, Ultimate 5.00 MPa
725 psi
GB/T 528
Chengdu Polyster 5500 General Grade TPV
Information provided by Chengdu Polyster Co., Ltd.
Tensile Strength, Ultimate 5.00 MPa
725 psi
GB/T 528
Chengdu Polyster FR2065 Flame Retardant Grade TPV
Good heat stability and light stability. Meets the requirements of European Dioxine Principle and the environmental protection criteria. Can be used for wires, cables, buncles, carcass of train.Inf..
Tensile Strength, Ultimate 5.00 MPa
725 psi
Dow Corning HV 1650/50 SILICONE RUBBER
50 Shore A hardness high consistency silicone rubber with excellent tracking and erosion resistance and low modulusInformation provided by Dow Corning
Tensile Strength, Ultimate 5.00 MPa
725 psi
Dow Corning SILASTIC® 9252/250P PARTS A&B
Information provided by Dow Corning
Tensile Strength, Ultimate 5.00 MPa
725 psi
In Plane Direction
Cymat A35620SC 040SS Stabilized Aluminum Foam
Description: Cymat A35620SC 040SS stabilized aluminum foam (SAF) is a closed cell aluminum foam formed from A356 aluminum alloy with a density of 0.4 g/cm3. The mechanical properties of SAF make it ..
Tensile Strength, Ultimate 5.00 - 14.0 MPa
725 - 2030 psi
ATG s.r.l. ACM Polyacrylic Rubber
Tensile Strength, Ultimate 5.00 - 17.0 MPa
725 - 2470 psi
ATG s.r.l. FPM Fluoroelastomer
Tensile Strength, Ultimate 5.00 - 34.5 MPa
725 - 5000 psi
Average value: 20.3 MPa Grade Count:29
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and ..
Tensile Strength, Ultimate 5.00 - 128 MPa
725 - 18500 psi
Average value: 28.2 MPa Grade Count:238
Overview of materials for Polypropylene Copolymer
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp..
Tensile Strength, Ultimate 5.00 - 15.0 MPa

@Temperature 60.0 - 90.0 °C
725 - 2180 psi

@Temperature 140 - 194 °F
Average value: 10.0 MPa Grade Count:1
Overview of materials for Polypropylene with 40% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are..