Material Notes:
Styrene-Butadiene CopolymerDescription: Finaprene® 411x is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its high molecular weight, Finaprene® 411x provides excellent mechanical and elastic properties to compound.Applications: Thanks to its high molecular weight Finaprene® 411x is designed for the compounding industry. This crumb shape, along with the high molecular weight confer a quick and important oil absorption capacity to the polymer and lead tot eh production of economical compounds while keeping good mechanical properties.Content of the compound for which the listed properties apply: F484: 90F435: 35F411X: 5Oil: 40GPPS: 20HIPS: 20CaCO3: 15Additional Notes: DIN Abrasion: 195 mm³Rossflex 100%: 35000 cyclesRossflex 300%: 70000 cyclesRossflex 500%: 92000 cyclesData provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Viscosity Measure 25 cSt
25 cSt
Toluene Solution; Finaprene 1008 Test
Melt Flow 53 g/10 min

@Load 5.00 kg,
Temperature 190 °C
53 g/10 min

@Load 11.0 lb,
Temperature 374 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 57
57
Finaprene 1505 Test
Tensile Strength, Ultimate 5.00 MPa
725 psi
ASTM D638
Elongation at Break 3.8 %
3.8 %
unusually low elongation - error in manufacturer testing?; ASTM D638
Flex Crack Resistance 35000
35000
cycles per Rossflex 100%
70000
70000
cycles per Rossflex 300%
92000
92000
cycles per Rossflex 500%
Abrasion 195
195
mm³; DIN Abrasion
Users viewing this material also viewed the following: