Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 47.0 MPa | 6820 psi | ASTM D638 |
PolyOne Lubri-Tech™ PS-000/15T Polyester (PBT) - 15% PTFE Lubricated
(discontinued **) Data provided by PolyOne. |
|||
Tensile Strength, Ultimate | 47.0 MPa | 6820 psi | ASTM D638 |
PolyOne Lubri-Tech™ PS-000/15T-2S Polyester (PBT) - 15% PTFE Lubricated - 2% Silicone Lubricated
(discontinue Data provided by PolyOne. |
|||
Tensile Strength, Ultimate | 47.0 MPa | 6820 psi | ASTM D638 |
Shell Carilon® DP R1000 Polyketone
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON® Thermoplastic Polymer DP R1000 is a high flow developmental engineering polyketone resin from Shell Chemi.. |
|||
Tensile Strength, Ultimate | 47.0 MPa | 6820 psi | ASTM D638 |
Kleerdex Kydex® P54 Acrylic/PVC Extrusion Compound
(discontinued **) High impact profile extrusion compoundApplications: Extruded profiles requiring high impact, good chemical resistance, weatherability, and excellent flammability resistance.Features: P54 is extremel.. |
|||
Tensile Strength, Ultimate | 47.0 - 105 MPa | 6820 - 15200 psi | Average value: 80.2 MPa Grade Count:72 |
Overview of materials for Nylon 66, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu.. |
|||
Tensile Strength, Ultimate | 47.0 MPa | 6820 psi | |
Kuraray HYBRAR® PS2 Thermoplastic Rubber-Polystyrene Blend Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |
|||
Tensile Strength, Ultimate | 47.0 MPa | 6820 psi | |
Lucite International Lucite® 4F Acrylic Bead Resin Lucite® 4F is used as a dental resin and for casting and embedment. It is a fine particle size resin. It is a methyl methacrylate homopolymer.General Lucite® Acrylic Bead Resin Information: .. |
|||
Tensile Strength, Ultimate | 47.0 MPa | 6820 psi | |
Lucite International Lucite® 4G Acrylic Bead Resin Lucite® 4G is usually processed as a glass separation resin and has a wider particle size distribution than grade 47G. It is a methyl methacrylate homopolymer.General Lucite® Acrylic Bead Res.. |
|||
Tensile Strength, Ultimate | 47.0 MPa | 6820 psi | ASTM D638 |
Hannam Chemical Hanalac 750 ABS, General Purpose FDA Approved. Good combination of impact strength, rigidity, gloss, heat resistance, processability, and thermal stability. May be injection molded. Its broad range of applications include: elect.. |
|||
Tensile Strength, Ultimate | 47.0 MPa | 6820 psi | DIN 53504 |
Lubrizol ESTANE® T5417 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 47.0 MPa | 6820 psi | ASTM D638 |
Plenco 08225 Polyester BMC, Compression Molded PLENCO 08225 is a renumber of PlasGlas 20215. PLENCO 08225 is a 15% glass-filled polyester bulk molding compound characterized as a medium strength electrical grade, but has many outstanding propert.. |
|||
Tensile Strength, Ultimate | 47.0 MPa | 6820 psi | ASTM D638 |
Plenco 1501 Polyester, Pellet, Injection Molded PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength va.. |
|||
Tensile Strength, Ultimate | 47.0 MPa | 6820 psi | ASTM D638 |
Plenco 4304 Phenolic, Nodular, Transfer Molded PLENCO 04304 is a heat resistant, mineral filled phenolic molding compound offering improved mechanical strength properties along with excellent dimensional stability. UL recognized under component .. |
|||
Tensile Strength, Ultimate | 47.0 MPa | 6820 psi | ISO 527-1, 2 |
Polyplastics Duranex® 6370B Polybutylene Terephthalate (PBT), Anisotropy improvement, 30% GB filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Tensile Strength, Ultimate | 47.0 MPa | 6820 psi | DIN 53504 |
Lubrizol ESTANE® 58277 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 47.0 MPa @Temperature 260 °C |
6820 psi @Temperature 500 °F |
ASTM D638 |
UBE UPIMOL® SA101 Heat-Resistant Polyimide Shape Description: UPIMOL® SA101 is an excellent heat-resistant polyimide shape, based on Biphenyl tetracarboxilic dianhydride(BPDA) originally developed by UBE. UPIMOL® SA101 has improved high durabili.. |
|||
Tensile Strength, Ultimate | 47.0 MPa | 6820 psi | ASTM D638 |
Toyobo Vylopet® EMC605 PET/PBT Blend Key Feature: Flame retardant V-0 UL 94 classApplications: glossy surface componentsPET/PBT blends suggested for glossy surfaces. General features of Vylopet® include heat resistance, good mechanic.. |
|||
Tensile Strength, Ultimate | 47.0 MPa | 6820 psi | ASTM D638 |
Eastman Tenite Butyrate 264E0096908 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 22%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Tensile Strength, Ultimate | 47.0 MPa | 6820 psi | ISO 527 |
DSM Fibre Intermediates Nyrim® 2000 (Dry) Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is processed via Reaction Injection Moulding (RIM) tec.. |
|||
Tensile Strength, Ultimate | 47.0 MPa | 6820 psi | ASTM D638 |
Cresset Powers Cress-Alon™ NE6040-ST 4% Nano Clay Loaded, 6.0 r.v. Super Tough Grade Nylon 6, Dry As Molded Surpasses super tough neat resins in strength, heat resistance, and hardness.Information provided by Cresset Powers Ltd. |
|||
Tensile Strength, Ultimate | 47.0 MPa | 6820 psi | ATSM D638 |
Ashley Polymers Ashlene® ABS Resin F-216 General purpose high impact resin.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 47.0 MPa | 6820 psi | ASTM D638 |
Toyobo A1064D Thermoplastic Polyurethane Elastomer, Injection Grade Polybutyleneadipate type, the most general purpose type of Toyobo Polyurethane; features excellent cost-performance. Various grades of Toyobo polyurethane TPEs are used in auto parts, hoses, tubes,.. |
|||
Tensile Strength, Ultimate | 47.0 - 117 MPa | 6820 - 17000 psi | Average value: 83.8 MPa Grade Count:8 |
Overview of materials for Polyphenylene Sulfide (PPS), Stainless Steel Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Stainless Steel Fiber". Each property range of values reported is minimum a.. |