Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 39.3 MPa | 5700 psi | |
Abatron AboCast 8-8/Abocure 8-8 Epoxy
(discontinued **) 2-part solvent-free dielectric epoxy casting compound.Processing: 100/50 ratio (pbw); Gel time, 1 lb. (2.2 kg): 135 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°C (212°F)... |
|||
Tensile Strength, Ultimate | 39.3 - 60.0 MPa | 5700 - 8700 psi | Average value: 53.1 MPa Grade Count:3 |
Overview of materials for Nylon 6/69 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6/69". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |
|||
Tensile Strength, Ultimate | 39.3 MPa | 5700 psi | ASTM D638-95 |
Multibase Multi-ABS 3365 High Impact ABS Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 39.3 MPa | 5700 psi | ASTM D638-95 |
Multibase Multi-ABS 802 Natural Extrusion Grade Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 39.3 MPa | 5700 psi | ASTM D638 |
Eastman Tenite Butyrate 264A3720013 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 13%. Weight loss on heating = 0.6% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Tensile Strength, Ultimate | 39.3 MPa | 5700 psi | |
Colorite Polymers 10013G-015 Clear Extrusion Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for the extrusion of various components for the production of devices. The vinyl components used in pre.. |
|||
Tensile Strength, Ultimate | 39.3 MPa | 5700 psi | |
Colorite Polymers 10014G-015 Clear Injection Molding Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for injection molding of various components such as drip chambers, connectors, valves, etc. The vinyl c.. |
|||
Tensile Strength, Ultimate | 39.3 MPa | 5700 psi | |
BCC Products Kwik Kast BC 8001 Urethane Casting BC8001 is an advanced fast cast polyurethane tooling system. It features low viscosity, low exotherm and minimal shrinkage. It cures hard, yet more durable resulting in less brittle parts. Designed.. |
|||
Tensile Strength, Ultimate | 39.3 MPa | 5700 psi | ASTM D638 |
Eastman Tenite Butyrate 465A3720010 Clear, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 10%. Weight loss on heating = 0.9% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |