Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 35.0 - 250 MPa @Temperature 60.0 - 275 °C |
5080 - 36300 psi @Temperature 140 - 527 °F |
Average value: 134 MPa Grade Count:14 |
Overview of materials for Polyetheretherketone, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
Tensile Strength, Ultimate | 35.0 - 117 MPa | 5080 - 17000 psi | Average value: 67.1 MPa Grade Count:28 |
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled". Each property range of values repor.. |
|||
Tensile Strength, Ultimate | 35.0 MPa | 5080 psi | ISO 527 |
LATI LASTANE 50 High Impact Polyurethane (PUR)
(Unverified Data**) Description: Lastane thermoplastics are polyurethane (PUR) products. They exhibit good wear and impact resistance, even at low temperatures, noise inertness and excellent mould release. These proper.. |
|||
Tensile Strength, Ultimate | 35.0 - 110 MPa | 5080 - 16000 psi | Average value: 55.1 MPa Grade Count:85 |
Overview of materials for Polycarbonate/PET Polyester Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values.. |
|||
Tensile Strength, Ultimate | 35.0 - 45.0 MPa | 5080 - 6530 psi | ASTM D638 |
Solvay Specialty Polymers Hylar® MP10 PVDF Polyvinylidene Fluoride
(discontinued **) Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a.. |
|||
Tensile Strength, Ultimate | 35.0 - 115 MPa @Temperature -40.0 - 100 °C |
5080 - 16700 psi @Temperature -40.0 - 212 °F |
Average value: 70.0 MPa Grade Count:1 |
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum .. |
|||
Tensile Strength, Ultimate | 35.0 MPa | 5080 psi | ISO 527 |
Solvay Technyl® A 246M Nylon 66, Impact Grade, EH50 Unreinforced and modified polyamide 66, with improved impact resistance, heat stabilized, for injection molding.Technyl A 246m offers an excellent notched impact resistance at low temperatures makin.. |
|||
Tensile Strength, Ultimate | 35.0 MPa | 5080 psi | 2 in/min, at max load; ASTM D638 |
A. Schulman POLYPUR™ FPU 1117 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 35.0 MPa | 5080 psi | at max load; ASTM D638 |
A. Schulman POLYPUR™ FPU 1376 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 35.0 MPa | 5080 psi | 2 in/min, at max load; ASTM D638 |
A. Schulman POLYPUR™ FPU 1117 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 35.0 MPa | 5080 psi | at max load; ISO 527 |
A. Schulman FORMION™ FI 131E Adhesive, Extrusion Grade DescriptionFormion® FI 131E is an adhesive grade extrusion product. It has been formulated to provide adhesion as a tie layer or resin modifier to bond Ionomer to polar and non polar substances, s.. |
|||
Tensile Strength, Ultimate | 35.0 MPa | 5080 psi | 2 in/min, at max load; ASTM D638 |
A. Schulman POLYPUR™ FPU 1117 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 35.0 MPa | 5080 psi | at max load; ASTM D638 |
A. Schulman POLYPUR™ FPU 1376 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 35.0 MPa | 5080 psi | at max load; ISO 527 |
A. Schulman FORMION™ FI 131E Adhesive, Extrusion Grade DescriptionFormion® FI 131E is an adhesive grade extrusion product. It has been formulated to provide adhesion as a tie layer or resin modifier to bond Ionomer to polar and non polar substances, s.. |
|||
Tensile Strength, Ultimate | 35.0 MPa | 5080 psi | at max load; ASTM D638 |
A. Schulman POLYPUR™ FPU 1376 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 35.0 MPa | 5080 psi | at max load; ISO 527 |
A. Schulman FORMION™ FI 131E Adhesive, Extrusion Grade DescriptionFormion® FI 131E is an adhesive grade extrusion product. It has been formulated to provide adhesion as a tie layer or resin modifier to bond Ionomer to polar and non polar substances, s.. |
|||
Tensile Strength, Ultimate | 35.0 MPa | 5080 psi | ISO 37 |
Lubrizol ESTANE® GP80AB Ester Based Thermoplastic Polyurethane Type: Estane® GP 80AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Tensile Strength, Ultimate | 35.0 MPa | 5080 psi | ISO 37 |
Lubrizol ESTANE® GP80AE Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 35.0 MPa | 5080 psi | ISO 527-1, 2 |
Polyplastics Duracon® TD-25 Acetal Co-polymer (POM), High impact, Flexible DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Tensile Strength, Ultimate | 35.0 MPa | 5080 psi | ISO 527-1 |
Chengdu Polyster H6055 Thermoplastic Polyether-ester Elastomer (TPEE) Medium modulus molding and injection grade. Contains improved color- stable antioxidants. Higher melt flow index compared with other grades; good balance of modulus and toughness. Applications requi.. |
|||
Tensile Strength, Ultimate | 35.0 MPa | 5080 psi | cond; ISO 527-1/-2 |
DSM Akulon® K222-KMV5 /A PA6-MD25 FR(30) 25% Mineral Reinforced, Flame Retardant (Halogen free), Color Stabilized |
|||
Tensile Strength, Ultimate | 35.0 MPa | 5080 psi | ISO 527-1/-2 |
DSM Arnitel® EM631 TPC-ET Extrusion Grade |
|||
Tensile Strength, Ultimate | 35.0 MPa | 5080 psi | ASTM D638 |
Chem Polymer Durlex 709 IH PBT, Impact Modified A highly impact modified PBT exhibiting excellent toughness and processability.Data provided by the manufacturer, Chem Polymer. |
|||
Tensile Strength, Ultimate | 35.0 - 45.0 MPa | 5080 - 6530 psi | ASTM D638 |
Solvay Specialty Polymers Hylar® MP20 PVDF Polyvinylidene Fluoride
(discontinued **) Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a.. |
|||
Tensile Strength, Ultimate | 35.0 MPa | 5080 psi | ASTM D638 |
Solvay Specialty Polymers Algoflon® F3140 X PTFE (Polytetrafluoroethylene)
(discontinued **) Data provided by the manufacturer.Type II Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric prope.. |
|||
Tensile Strength, Ultimate | 35.0 - 100 MPa @Temperature -40.0 - 70.0 °C |
5080 - 14500 psi @Temperature -40.0 - 158 °F |
Average value: 67.5 MPa Grade Count:4 |
Overview of materials for Acrylic, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |