Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 30.0 MPa | 4350 psi | ASTM D638 |
NCMT NanoPAC™ G2030I High Performance Polypropylene Nanocomposite Applications: Construction MaterialInformation provided by Nano Composite Materials Technology Limited |
|||
Tensile Strength, Ultimate | 30.0 MPa | 4350 psi | ISO 527-2 |
NOVA Chemicals DYLARK® 378 Impact Grade Engineering Resin Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn.. |
|||
Tensile Strength, Ultimate | 30.0 MPa | 4350 psi | ISO 527 |
LATI LASTIROL R-V0 Polystyrene (PS) (UL94 V-0)
(discontinued **) Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass fiber reinforc.. |
|||
Tensile Strength, Ultimate | 30.0 MPa | 4350 psi | ISO 527 |
LATI LASTIROL TR-V0 Polystyrene (PS) (UL94 V-0)
(discontinued **) Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f.. |
|||
Tensile Strength, Ultimate | 30.0 - 50.0 MPa | 4350 - 7250 psi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 21508 PVDF Copolymer
(discontinued **) Key features of this grade: High Elongation, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® P.. |
|||
Tensile Strength, Ultimate | 30.0 - 147 MPa | 4350 - 21300 psi | Average value: 73.2 MPa Grade Count:90 |
Overview of materials for Nylon 6, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Tensile Strength, Ultimate | 30.0 - 299 MPa | 4350 - 43400 psi | Average value: 219 MPa Grade Count:91 |
Overview of materials for Nylon 66, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. .. |
|||
Tensile Strength, Ultimate | 30.0 MPa @Temperature 1204 °C |
4350 psi @Temperature 2199 °F |
|
Haynes HR-160® alloy, hot rolled and solution annealed plate Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Tensile Strength, Ultimate | 30.0 MPa | 4350 psi | DIN 53504 |
Lubrizol ESTANE® T5090 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 30.0 MPa | 4350 psi | ASTM D638 |
Tipco Tipcolite® THD 411 Phenolic Compound, Mica, Asbestos & Cellulose, Medium Flow & High Electrical Properties Medium Flow Phenolic Compound, Reinforced with Mica, Asbestos & CelluloseApplications: Electrical & ElectronicsProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Industr.. |
|||
Tensile Strength, Ultimate | 30.0 MPa | 4350 psi | ISO 37 |
Lubrizol ESTANE® GP75AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 75AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Tensile Strength, Ultimate | 30.0 MPa | 4350 psi | DIN 53504 |
Lubrizol ESTANE® 58370 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 30.0 MPa | 4350 psi | ISO 527-1 |
Chengdu Polyster FH605 Thermoplastic Polyether-ester Elastomer (TPEE) Blend of H605 and self-made flame retardant material. Flame retardant, high tear resistance. Applications requiring flame retardancy, such as wires, cables and optical fiber.Information provided by .. |
|||
Tensile Strength, Ultimate | 30.0 - 32.0 MPa | 4350 - 4640 psi | UV Postcure; ASTM D638M |
DSM Somos® 9120 The need for movable parts is a constant when it comes to prototyping. Being able to ensure the proper fit for parts within a component can save both time and money. Somos® 9120 creates semi-transp.. |
|||
Tensile Strength, Ultimate | 30.0 MPa | 4350 psi | ASTM D638 |
Eastman Eastar GN071 Natural PETG Copolyester EASTAR GN071 Copolyester is used for injection molding applications. It is sparkling clear, tough, chemical resistant, odor free, versatile, easy to work with and affordable. Cleaning solutions wi.. |
|||
Tensile Strength, Ultimate | 30.0 MPa | 4350 psi | ASTM D412 |
BASF Elastollan® 1175AW Polyether Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes... |
|||
Tensile Strength, Ultimate | 30.0 MPa | 4350 psi | ASTM D412 |
BASF Elastollan® C-70AW Polyester Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellen.. |
|||
Tensile Strength, Ultimate | 30.0 - 80.0 MPa | 4350 - 11600 psi | |
Alliance BIF-11 Bonded (Composite) Magnetic Material |
|||
Tensile Strength, Ultimate | 30.0 - 80.0 MPa | 4350 - 11600 psi | |
Alliance BIF-2 Bonded (Composite) Magnetic Material |
|||
Tensile Strength, Ultimate | 30.0 MPa | 4350 psi | ASTM D638 |
A. Schulman ComAlloy Voloy® 110 Polypropylene, Mineral Reinforced, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.15% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Ultimate | 30.0 MPa | 4350 psi | ASTM D638 |
Toyobo Pelprene™ S-1001 Polyester TPE Key Feature: Pelprene S typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'S' type is a block.. |
|||
Tensile Strength, Ultimate | 30.0 - 170 MPa @Temperature -20.0 - 150 °C |
4350 - 24700 psi @Temperature -4.00 - 302 °F |
Average value: 104 MPa Grade Count:1 |
Overview of materials for Nylon 6, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Tensile Strength, Ultimate | 30.0 MPa | 4350 psi | DIN 53504 |
Lubrizol ESTANE® 54630 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 30.0 - 35.9 MPa | 4350 - 5210 psi | Average value: 33.9 MPa Grade Count:3 |
Overview of materials for Polypropylene, Sheet/Thermoforming Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Sheet/Thermoforming Grade". Each property range of values reported is minimum and maximum.. |
|||
Tensile Strength, Ultimate | 30.0 - 65.0 MPa @Temperature 60.0 - 150 °C |
4350 - 9430 psi @Temperature 140 - 302 °F |
Average value: 46.3 MPa Grade Count:1 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min.. |