Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 4210 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 29.0 MPa
4210 psi
ASTM D638-95
Multibase Multi-Flex® TPO D-6500
Multi-Flex® D 6500 is well suited for TPO extrusion applications and certain high value molded parts for the telecommunications industry.Data provided by Multibase.
Tensile Strength, Ultimate 29.0 MPa
4210 psi
ASTM D638
NCMT NanoPAC™ HG500 High Performance Polypropylene Nanocomposite
Applications: Household Industry Electrical AppliancesInformation provided by Nano Composite Materials Technology Limited
Tensile Strength, Ultimate 29.0 - 147 MPa
4210 - 21300 psi
Average value: 70.3 MPa Grade Count:77
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an..
Tensile Strength, Ultimate 29.0 MPa
4210 psi
ASTM D638
Rotuba MS Cellulose Acetate
Property values at 50% RH.Data provided by the manufacturer.
Tensile Strength, Ultimate 29.0 MPa
4210 psi
ASTM D638
North Wood Plastics PS with 40% Wood Fiber
Data provided by North Wood Plastics, Inc.
Tensile Strength, Ultimate 29.0 MPa

@Temperature 90.0 °C
4210 psi

@Temperature 194 °F
ISO 527
LATI LATILUB 73/13-01M Polyoxymethylene Base (POM), 1% Molybdenum Disulfide Self Lubricating Plastic  (Unv
Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri..
Tensile Strength, Ultimate 29.0 MPa

@Temperature 60.0 °C
4210 psi

@Temperature 140 °F
ISO 527
LATI LATILUB 73/13-20T Polyoxymethylene Base (POM), 10% Mixed PTFE Self Lubricating Plastic  (Unverified D
Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri..
Tensile Strength, Ultimate 29.0 - 138 MPa
4210 - 20000 psi
Average value: 72.7 MPa Grade Count:55
Overview of materials for Polycarbonate, Stainless Steel Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Stainless Steel Fiber". Each property range of values reported is minimum and maximum val..
Tensile Strength, Ultimate 29.0 - 40.0 MPa
4210 - 5800 psi
Average value: 34.4 MPa Grade Count:16
Overview of materials for High Density Polyethylene (HDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max..
Tensile Strength, Ultimate 29.0 MPa
4210 psi
ASTM D638
DuPont™ Surlyn® 8527 Ionomer Resin, Sodium  (discontinued **)
Surlyn® 8527 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu..
Tensile Strength, Ultimate 29.0 MPa
4210 psi
Vulcanized
KKPC KOSYN 1500NF Styrene Butadiene Rubber
Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and..
Tensile Strength, Ultimate 29.0 MPa
4210 psi
ASTM D638
LyondellBasell Astryn 65F4-2 Polypropylene Homopolymer, 20% Talc
Key Features: conventional melt flow, high modulus, mineral-filled polypropylene homopolymer, excellent impact and stiffness balance, good dimensional stability, excellent heat resistance, good colo..
Tensile Strength, Ultimate 29.0 MPa
4210 psi
ASTM Data
Styron Magnumâ„¢ 9043 ABS, High Gloss Sheet Extrusion Grade
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Tensile Strength, Ultimate 29.0 MPa
4210 psi
ASTM D638
Elastomer Engineering Elastamide 300 Elastomer Modified RIM Nylon 6
22% crystallinity. Information supplied by Elastomer Engineering.
Tensile Strength, Ultimate 29.0 MPa
4210 psi
ASTM D638
Total PPR 7525MZ Polypropylene, Injection Molding Grade
Clarified random copolymer for injection moldingClarity - FINA 7525MZ exhibits superior clarity in molded parts.Impact - FINA 7525MZ produces molded parts with improved impact compared with parts mo..
Tensile Strength, Ultimate 29.0 MPa
4210 psi
ISO 37
Lubrizol ESTANE® 58280 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Tensile Strength, Ultimate 29.0 MPa
4210 psi
ASTM D638/D412
Covestro Bayflex® XGT-140 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System
0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of..
Tensile Strength, Ultimate 29.0 MPa
4210 psi
ISO 527
DSM Fibre Intermediates Nyrim® 3000 (Conditioned)
Conditioned at 23°C and 50% Relative Humidity.Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is proc..
Tensile Strength, Ultimate 29.0 MPa
4210 psi
Die C (35 min / 145°C); ASTM D412
Dow Buna® SB 1502 Cold polymerized Emulsion Styrene Butadiene Rubber (E-SBR)
Buna® SB 1502 - Schkopau is manufactured by cold polymerization using mixed rosin acid / fatty acid soaps. A non-discoloring stabilizer is added during the production process. Buna® SB 1502 - Sc..
Tensile Strength, Ultimate 29.0 MPa
4210 psi
3M Jet-Weld™ TE-100 Adhesive
A warm applied, moisture-curing polyurethane adhesive for wood working, laminating and plastic component assembly. Extrudable grade with medium set time and low viscosity ideal for bonding wood. Ca..
Tensile Strength, Ultimate 29.0 MPa
4210 psi
ASTM D638
A. Schulman ComAlloy Comshield® 104 Homopolymer Polypropylene, Electrically Conductive - Carbon Black Filled
Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line.
Tensile Strength, Ultimate 29.0 MPa
4210 psi
ASTM D638
Buckeye Polymers BP RPP 3019 TU Polypropylene, 30% Mineral Filled
UV StabilizedThis Talc-filled product exhibits excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and mar resistan..
Tensile Strength, Ultimate 29.0 MPa
4210 psi
ASTM D638
Devcon Wear Guard (High Load) Epoxy
Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives.
Tensile Strength, Ultimate 29.0 - 75.0 MPa
4210 - 10900 psi
Average value: 58.4 MPa Grade Count:31
Overview of materials for Acrylic, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
Tensile Strength, Ultimate 29.0 - 80.0 MPa

@Temperature -40.0 - 120 °C
4210 - 11600 psi

@Temperature -40.0 - 248 °F
Average value: 45.0 MPa Grade Count:4
Overview of materials for Nylon 6, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri..
Tensile Strength, Ultimate 29.0 MPa
4210 psi
ASTM Data
Americas Styrenics Styron® 425 High Impact Polystyrene  (discontinued **)
STYRON® 425 impact polystyrene resin is typically used in thin section parts, hot drink cups and cassettes. It offers heat resistance, easy flow, fast cycling, and excellent tensile and flex proper..
Tensile Strength, Ultimate 29.0 MPa
4210 psi
ISO 37
Lubrizol ESTANE® 58238 Ester Based Thermoplastic Polyurethane (European Grade)
Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability in a flexible..
Tensile Strength, Ultimate 29.0 - 39.0 MPa
4210 - 5660 psi
ISO 527
BASF Ecovio® C2203 F Blend Biodegradable Polyester
Description: Ecovio® F Blend C2203 is our biodegradable film product containing renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic aci..
Tensile Strength, Ultimate 29.0 - 153 MPa
4210 - 22200 psi
Average value: 101 MPa Grade Count:42
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported..