Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 280 MPa | 40600 psi | 0°; ASTM D3039 |
Polystrand ThermoPro™ IE6010 Unitape Unidirectional Polypropylene-Glass Composite Fiber Orientation is 0°.Polystrand ThermoPro™ combines continuous E-Glass (ThermoPro-E™) structural reinforcing fibers in either a polyethylene or polypropylene proprietary thermoplastic polymer .. |
|||
Tensile Strength, Ultimate | 280 - 450 MPa | 40600 - 65300 psi | |
Materion Brush 1915â„¢ Hard Temper Wire, 0.375" - 0.500" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Tensile Strength, Ultimate | >= 280 MPa | >= 40600 psi | |
H.C. Starck MoCu 65/35 Molybdenum-Copper Composite Material Description of Product: Molybdenum-copper composite materials are produced by copper infiltration of porous sintered molybdenum. They are available with different copper contents (15 - 35 %). A t.. |
|||
Tensile Strength, Ultimate | 280 - 450 MPa | 40600 - 65300 psi | |
Materion Brush 1915â„¢ Hard Temper Rod, 0.375" - 0.500" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Tensile Strength, Ultimate | 280 MPa | 40600 psi | |
Sapco 99.7% Aluminum Oxide Information provided by Sapco. |
|||
Tensile Strength, Ultimate | 280 MPa | 40600 psi | |
Ametek P410L P/M Stainless Steel, Sintered from 6.0 g/cc Green Density Powder apparent bulk density 2.8 g/cc; powder flow 30 sec/50g.Compacting properties measured on powders with 1% lithium stearite. Sintering was done in dissociated ammonia at 1121°C (2050°F) for .. |
|||
Tensile Strength, Ultimate | 280 - 360 MPa | 40600 - 52200 psi | |
ArcelorMittal 03 High formability steel for drawing, Cold rolled Available in the following: uncoated (DC01) and electroglavanized (DC01+ZE) Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These product.. |
|||
Tensile Strength, Ultimate | 280 - 340 MPa | 40600 - 49300 psi | |
ArcelorMittal 04 High formability steel for drawing, Cold rolled Available in the following: uncoated (DC04) and electroglavanized (DC04+ZE) Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These product.. |
|||
Tensile Strength, Ultimate | 280 MPa | 40600 psi | |
Ametek P303L P/M Stainless Steel, Sintered from 6.23 g/cc Green Density Powder apparent bulk density 2.8 g/cc; powder flow 30 sec/50g.Compacting properties measured on powders with 1% lithium stearate. Sintering was done in dissociated ammonia at 1121°C (2050°F) for .. |
|||
Tensile Strength, Ultimate | 280 MPa | 40600 psi | |
Ametek P304L P/M Stainless Steel, Sintered from 6.25 g/cc Green Density Powder apparent bulk density 2.7 g/cc; powder flow 30 sec/50g.Compacting properties measured on powders with 1% lithium stearite. Sintering was done in dissociated ammonia at 1121°C (2050°F) for .. |
|||
Tensile Strength, Ultimate | 280 - 360 MPa | 40600 - 52200 psi | |
ArcelorMittal 53 High formability steel for drawing, Cold rolled Available in the following: Extragal®/Galvannealed (DX53D +Z/+ZF)Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These products are used.. |
|||
Tensile Strength, Ultimate | 280 - 340 MPa | 40600 - 49300 psi | |
ArcelorMittal 54 High formability steel for drawing, Cold rolled Available in the following: Extragal®/Galvannealed (DX54D +Z/+ZF)Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These products are used.. |
|||
Tensile Strength, Ultimate | 280 MPa @Temperature 980 °C |
40600 psi @Temperature 1800 °F |
|
Haynes 242® alloy, hot rolled plate, annealed and aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good thermal.. |