Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 200 MPa | 29000 psi | ASTM D638 |
Owens Corning Glass Fiber Reinforced Polyester (Pultruded), 55 wt.% glass Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u.. |
|||
Tensile Strength, Ultimate | 200 MPa | 29000 psi | |
Pacific Sintered Materials F-241-S1 Iron Soft Magnetic Powdered Metal Applications: DC magnetic applications such as pole pieces, cores, armatures, generator rotors and stator cores.Equivalent ASTM Specification: B310-70, TYPE III, CLASS AAll information provided by P.. |
|||
Tensile Strength, Ultimate | 200 MPa | 29000 psi | |
PSM Industries Pacific Sintered Metals Iron F-241-S1 Powdered Metal DC magnetic applications such as pole pieces, cores, armatures, generator rotors and stator cores Equivalent ASTM Spec: B310-70, Type III, Class AInformation Provided by Pacific Sintered Metals, a .. |
|||
Tensile Strength, Ultimate | 200 MPa | 29000 psi | |
Parkway Products Thixomolded® AM50A Magnesium Thixomolding® is a fabrication technique, similar to injection molding, that uses magnesium alloys as the “resin” instead of plastic. Solid magnesium alloy pellets are fed into the machine, heate.. |
|||
Tensile Strength, Ultimate | 200 MPa | 29000 psi | ASTM D638 |
PTS Trimid® N66-G33HL 33% Glass Fiber Reinforced Heat Stabilized, Lubed Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Ultimate | 200 MPa | 29000 psi | ASTM D638 |
PTS Trimid® N66-G33L 33% Glass Fiber Reinforced Lubed Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Ultimate | 200 MPa | 29000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® NL-50GF/000 Black 13 Nylon 6/12, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedHeat StabilizedBlackNylon 6/12 CompoundDry as Molded:PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 200 MPa | 29000 psi | ASTM value at 5mm/min. |
BASF Capron® 5233G HS BK-102 33% Glass-Filled Nylon 66 (Dry)
(discontinued **) Capron 5233G HS BK-102 is a 35% glass reinforced, heat stabilized, pigmented black nylon 6,6 injection molding compound offering excellent strength, rigidity, stiffness, creep resistance, and dimens.. |
|||
Tensile Strength, Ultimate | 200 MPa @Temperature 982 °C |
29000 psi @Temperature 1800 °F |
|
Haynes 556® alloy, all-weld metal GTAW Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Tensile Strength, Ultimate | 200 MPa | 29000 psi | |
Wieland 1701 Wilaform Gold Yield alloy particularly suitable for coin and medal production. Also can be welded into platinum suitably.Applications: coin/shapeDental |
|||
Tensile Strength, Ultimate | 200 MPa | 29000 psi | ASMT D638 |
Toyobo TS501 PPS, 50% Glass Fiber Reinforced Key Feature: High stiffnessHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo. Excellent physical, e.. |
|||
Tensile Strength, Ultimate | 200 MPa | 29000 psi | dry; ISO 527-1/-2 |
DSM Akulon® N24-G8 PA6-GF40 40% Glass Reinforced |
|||
Tensile Strength, Ultimate | 200 MPa @Temperature 871 °C |
29000 psi @Temperature 1600 °F |
|
Crucible Steel 20 Cb Plus Stainless Steel Crucible 20 Cb Plus is a non-hardenable stabilized stainless steel with exceptional resistance to sulfuric, phosphoric, and nitric acid. This grade also has good resistance to stress corrosion crack.. |
|||
Tensile Strength, Ultimate | 200 MPa | 29000 psi | |
China Tungsten STG30-20 PM Structural Parts Information provided by China Tungsten |
|||
Tensile Strength, Ultimate | 200 MPa | 29000 psi | |
China Tungsten STG60-20 PM Structural Parts Information provided by China Tungsten |
|||
Tensile Strength, Ultimate | 200 MPa | 29000 psi | |
China Tungsten STG90-20 PM Structural Parts Information provided by China Tungsten |
|||
Tensile Strength, Ultimate | 200 MPa | 29000 psi | Annealed |
CMW® D154X Post-Oxidized Silver Cadmium Oxide Contact Material ASTM B781 Table 3 For electrical contacts; resistant to welding and high surge currents.Information provided by CMW Inc. |
|||
Tensile Strength, Ultimate | 200 MPa | 29000 psi | ISO 527-1/-2 |
DSM Arnite® AV2 370 HF PET-GF35 35% Glass Reinforced, Brake Booster Body Valves, High Flow |
|||
Tensile Strength, Ultimate | 200 MPa | 29000 psi | |
China Tungsten STG10-20 PM Structural Parts Information provided by China Tungsten |
|||
Tensile Strength, Ultimate | 200 MPa @Temperature 871 °C |
29000 psi @Temperature 1600 °F |
|
Carpenter 20Cb-3® Stainless Steel Data provided by Carpenter Technology Corporation.20Cb-3® is an austenitic stainless steel possessing excellent resistance to hot sulfuric acid and many other aggressive environments which would re.. |
|||
Tensile Strength, Ultimate | 200 MPa | 29000 psi | 10 oz glass cloth laminate |
BCC Products BC 5105 Epoxy Laminating System BC 5105 is a clear, unfilled, low viscosity laminating system. This heat resistant resin exhibits excellent wet out, reasonable working time and may be used at room temperature without post-curing. .. |
|||
Tensile Strength, Ultimate | 200 - 241 MPa | 29000 - 35000 psi | Annealed Sheet |
ATI Wah Chang Vanadium Vanadium is widely dispersed in the earths crust occurring in many types of deposits. Most vanadium is currently obtained as a by-product or co product from titanomagnetites, petroleum, uranium ores.. |
|||
Tensile Strength, Ultimate | 200 - 331 MPa | 29000 - 48000 psi | Average value: 264 MPa Grade Count:14 |
Overview of materials for Nylon 66, 40% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Carbon Fiber Filled". Specific grades with carbon fiber content between 35% and 44% are in.. |