Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 20.0 MPa | 2900 psi | X direction; 0.1/min strain rate; ASTM D638 |
Rogers Corporation RT/duroid® 6006 Ceramic-PTFE Composite Microwave Laminate Features:High dielectric constant for circuit size reductionLow loss - Ideal for operating at X-band or belowTight dielectric constant and thickness control for repeatable circuit performanceLow moi.. |
|||
Tensile Strength, Ultimate | 20.0 MPa | 2900 psi | ASTM D638 |
NCMT NanoPAC™ HG537 High Performance Polypropylene Nanocomposite Applications: Household Industry Electrical AppliancesInformation provided by Nano Composite Materials Technology Limited |
|||
Tensile Strength, Ultimate | 20.0 MPa | 2900 psi | ASTM D638 |
NCMT NanoPAC™ S202 High Performance Polypropylene Nanocomposite Characteristics: High stiffness Supplementary of ABS Good impact resistant Less shrinkage Good thermal conductivity Applications: Toys Industry AutomobileInformation provided by Nano Composite Mater.. |
|||
Tensile Strength, Ultimate | 20.0 MPa | 2900 psi | ASTM D638 |
NCMT NanoPAC™ S212 High Performance Polypropylene Nanocomposite Characteristics: High stiffness Supplementary of ABS Good impact resistant Less shrinkage Good thermal conductivity Applications: Toys Industry AutomobileInformation provided by Nano Composite Mater.. |
|||
Tensile Strength, Ultimate | 20.0 MPa | 2900 psi | ASTM D638 |
NCMT NanoPAC™ S222 High Performance Polypropylene Nanocomposite Characteristics: High stiffness Supplementary of ABS Good impact resistant Less shrinkage Good thermal conductivity Applications: Toys Industry AutomobileInformation provided by Nano Composite Mater.. |
|||
Tensile Strength, Ultimate | 20.0 MPa | 2900 psi | ISO 527 |
Premix Thermoplastics PRE-ELEC® PP 1373 PRE-ELEC PP 1373 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Tensile Strength, Ultimate | 20.0 MPa | 2900 psi | ASTM D638 |
North Wood Plastics PS with 20% Wood Fiber Data provided by North Wood Plastics, Inc. |
|||
Tensile Strength, Ultimate | 20.0 - 20.0 MPa @Temperature 60.0 - 60.0 °C |
2900 - 2900 psi @Temperature 140 - 140 °F |
Average value: 20.0 MPa Grade Count:1 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor.. |
|||
Tensile Strength, Ultimate | 20.0 - 65.0 MPa @Temperature 60.0 - 150 °C |
2900 - 9430 psi @Temperature 140 - 302 °F |
Average value: 45.8 MPa Grade Count:4 |
Overview of materials for Nylon 66, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu.. |
|||
Tensile Strength, Ultimate | 20.0 MPa @Temperature 22.0 °C |
2900 psi @Temperature 71.6 °F |
25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® BMC 2310 Unsaturated Polyester UP BMC 2310 is a chemically resistant grade reinforced with special fibres. Being completely glass-free (no glass fibre reinforcement) it is specifically recommended for the manufacture of high voltage.. |
|||
Tensile Strength, Ultimate | 20.0 MPa | 2900 psi | at max load; ISO 527 |
A. Schulman FORMION™ FI 391 Ionomer DescriptionFormion® FI 391 is a non-reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, low temperature ductility, and medium stiffness. Formion F1 391U i.. |
|||
Tensile Strength, Ultimate | 20.0 MPa | 2900 psi | at max load; ISO 527 |
A. Schulman FORMION™ FI 391 Ionomer DescriptionFormion® FI 391 is a non-reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, low temperature ductility, and medium stiffness. Formion F1 391U i.. |
|||
Tensile Strength, Ultimate | 20.0 MPa | 2900 psi | |
Williams Advanced Alloys WS243 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Tensile Strength, Ultimate | 20.0 MPa | 2900 psi | at max load; ISO 527 |
A. Schulman FORMION™ FI 391 Ionomer DescriptionFormion® FI 391 is a non-reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, low temperature ductility, and medium stiffness. Formion F1 391U i.. |
|||
Tensile Strength, Ultimate | 20.0 MPa | 2900 psi | DIN 53504 |
Lubrizol ESTANE® 58564 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 20.0 MPa | 2900 psi | ASTM D638 |
Eastman Tenite Butyrate 565A3720023 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 23%. Weight loss on heating = 1.2% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Tensile Strength, Ultimate | 20.0 - 50.0 MPa | 2900 - 7250 psi | |
Alliance C-7B Strontium Ferrite Ceramic Magnetic Material |
|||
Tensile Strength, Ultimate | 20.0 - 50.0 MPa | 2900 - 7250 psi | |
Alliance C-9 Strontium Ferrite Ceramic Magnetic Material |
|||
Tensile Strength, Ultimate | 20.0 MPa | 2900 psi | ASTM D638 |
A. Schulman ComAlloy Comtuf® 152 Polypropylene, Mineral Reinforced, Impact Modified Data provided by the manufacturer, ComAlloy International Company.20% Mineral Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been i.. |
|||
Tensile Strength, Ultimate | 20.0 MPa | 2900 psi | ASTM D638 |
Solvay Specialty Polymers Algoflon® 50 INOX PTFE; Stainless Steel Filled
(discontinued **) Data provided by the manufacturer.50 wt.% Stainless Steel. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric properties, a.. |
|||
Tensile Strength, Ultimate | 20.0 - 52.4 MPa | 2900 - 7600 psi | Average value: 36.3 MPa Grade Count:88 |
Overview of materials for Cellulose Acetate Butyrate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Butyrate, Molded". Each property range of values reported is minimum and maximum value.. |
|||
Tensile Strength, Ultimate | 20.0 MPa | 2900 psi | DIN 53504 |
Lubrizol ESTANE® 58244 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 20.0 - 52.0 MPa @Temperature -18.0 - 90.0 °C |
2900 - 7540 psi @Temperature -0.400 - 194 °F |
Average value: 35.8 MPa Grade Count:3 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma.. |
|||
Tensile Strength, Ultimate | 20.0 - 46.0 MPa | 2900 - 6670 psi | Average value: 37.5 MPa Grade Count:16 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum.. |
|||
Tensile Strength, Ultimate | 20.0 MPa | 2900 psi | ASTM D638 |
Multibase Multi-Flam™ 1502 PP Black Polypropylene Features:Flame Retardant Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Tensile Strength, Ultimate | 20.0 MPa | 2900 psi | DIN 53455 |
Ineos Nova S-3207 Medium Impact Compact Polystyrene
(discontinued **) High flow medium impact polystyrene, designed of injection molding of low friction household goods, packaging and toys. It combines low friction properties with excellent (ultrasonic) weldability.A.. |