Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 93.1 MPa | 13500 psi | ASTM D638 |
Nylene® Vexel™ B12GF15 SA , 15% Glass Reinforced PBT Description: Vexel™ B12GF15 SA is a 15% glass fiber reinforced PBT with improved surface aPolyphenylene Etherarance. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are.. |
|||
Tensile Strength, Ultimate | 93.2 MPa | 13500 psi | DIN 53455; ASTM D638 |
Kolon SPESIN® KP2122G15VO G/F Reinforced & Retardant PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
Tensile Strength, Ultimate | 93.0 MPa | 13500 psi | ASTM D638 |
Solvay Specialty Polymers Amodel® A-1240 HS Polyphthalamide (PPA) Resin, 40% Mineral Reinforced, at 50% RH
(d AMODEL A-1240 polyphthalamide (PPA) resins are 40% mineral filled resins that have high deflection temperature, flexural modulus, and tensile strength. They mold with low warpage, have excellent di.. |
|||
Tensile Strength, Ultimate | 93.0 MPa | 13500 psi | ASTM D638 |
PolyOne Edgetek® ES-15GF/000 RED Polyethersulfone - 15% Glass Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Tensile Strength, Ultimate | 93.1 MPa | 13500 psi | |
XX Phenolic Laminate Paper based phenolic provides low cost electrical and mechanical properties. It is widely used for switchboards, panel boards, insulating washers, and intricate punched parts.Information provided b.. |
|||
Tensile Strength, Ultimate | 93.1 MPa | 13500 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ NL-20GF/05T Nylon 6/12, Glass Filled, PTFE Lubricated
(discontinued **) Description/Features:Glass Fiber ReinforcedPTFE LubricatedInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 93.2 MPa | 13500 psi | DIN 53455; ASTM D638 |
Kolon KOLEFIN® KO133GM40 M/F Reinforced Polypropylene KOLEFIN® has excellent mechanical properties and its cost is lower than other engineering plastics. KOLEFIN® is widely used in the automotive industry and business applications.Good mechanica.. |
|||
Tensile Strength, Ultimate | 93.2 MPa | 13500 psi | DIN 53455; ASTM D638 |
Kolon KOPA® KN333MS Low Friction Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Tensile Strength, Ultimate | 93.4 MPa | 13500 psi | ISO 527-1, 2 |
Polyplastics Duranex® CRN7015 Polybutylene Terephthalate (PBT), Low gas generation, Low contact contamination, FR, UL approved regrind 50%, 15% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Tensile Strength, Ultimate | 93.0 MPa | 13500 psi | ASTM D638 |
Plenco 6401 Phenolic, Briquette, Injection Molded PLENCO 06401 is a glass fiber and mineral filled two-stage phenolic molding compound. UL recognized under component file E40654. 06401 is available in black.Information supplied by Plenco. |
|||
Tensile Strength, Ultimate | 93.0 MPa | 13500 psi | ISO 527-1, 2 |
Polyplastics Duranex® 711SA Polybutylene Terephthalate (PBT), Low density, Low wear, GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Tensile Strength, Ultimate | 93.0 MPa | 13500 psi | ISO 527-2/1A/5 |
Lubrizol ESTALOC® 59600 Ester-Type, Reinforced Engineering Thermoplastic (European Grade) Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio.. |
|||
Tensile Strength, Ultimate | 93.1 MPa | 13500 psi | ASTM D638 |
Adell BT-13 Nylon 6, 15% Glass Reinforced; Impact Modified Data provided by Adell Plastics, Inc. |
|||
Tensile Strength, Ultimate | 93.1 MPa | 13500 psi | ASTM D638 |
Adell BT-33 Nylon 6, 15% Glass Reinforced; Impact Modified Data provided by Adell Plastics, Inc. |
|||
Tensile Strength, Ultimate | 93.0 MPa | 13500 psi | 5mm/min; ISO 527 |
BASF Ultradur B 4300 G3 15% Glass Filled PBT Ultradur B 4300 G3 is an easy flowing injection molding PBT with 15% glass fiber reinforcement for rigid, tough, and dimensionally stable parts. |
|||
Tensile Strength, Ultimate | 93.0 MPa | 13500 psi | ATSM D638 |
Ashley Polymers Ashlene® 925L-25G Nylon 12, 25% Glass Reinforced A 25% glass reinforced Nylon 12 resin for injection molding.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 93.0 MPa | 13500 psi | ATSM D638 |
Ashley Polymers Ashlene® P124WO PBT Polyester, 20% Glass Reinforced Flame retardant 20% glass reinforced, natural. Colors will modify properties.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 93.0 MPa | 13500 psi | ASTM D638 |
Chem Polymer Chemlon 206 G Nylon 6, 6% Glass Fiber Reinforced A 6% glass fiber reinforced nylon 6 offering improved creep resistance, stiffness, tensile and dimensional stability over unmodified nylon 6 materials.Data provided by the manufacturer, Chem Polymer.. |
|||
Tensile Strength, Ultimate | 93.0 MPa | 13500 psi | ASTM D638 |
Chem Polymer Chemlon 217 GI Nylon 6, 17% Glass Fiber Reinforced A 17% glass fiber reinforced, impact modified nylon 6 offering a combination of creep resistance, stiffness and toughness over unmodified nylon 6 materials.Data provided by the manufacturer, Chem Po.. |
|||
Tensile Strength, Ultimate | 93.0 MPa | 13500 psi | ASTM D638 |
A. Schulman ComAlloy Hiloy® 223 ABS, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Ultimate | 93.0 MPa | 13500 psi | ASTM D638 |
A. Schulman ComAlloy Hiloy® 243 SAN, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Ultimate | 93.0 MPa | 13500 psi | ATSM D638 |
Ashley Polymers Ashlene® 925LS-23G Nylon 12, 23% Glass Reinforced A 23% glass reinforced Nylon 12 resin, with heat stabilizer, for injection molding.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 93.0 MPa | 13500 psi | ASTM D638 |
A. Schulman ComAlloy Comtuf® 462 Glass/Mineral Reinforced, PET Alloy, Impact Modified, UL Data provided by the manufacturer, ComAlloy International Company.50% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Ultimate | 93.0 MPa | 13500 psi | ATSM D638 |
Ashley Polymers Ashlene® 124 PBT Polyester, 20% Glass Reinforced General purpose 20% glass reinforcement, natural. Colors will modify properties.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 93.0 MPa | 13500 psi | 5mm/min; ISO 527 |
BASF Ultramid® TG3S BK-104 15% Glass Filled PA6 (Dry) Ultramid TG3S BK-104 is a 15% glass reinforced, heat stabilized, impact modified PA6 injection molding compound developed for applications requiring improved toughness in combination with a balance .. |