Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ASTM D638 |
Plaskolite Optix® CA-75 General Purpose Acrylic Resin Injection Molding and Extrusion Grade Pellets. Highest heat resistance, medium flow. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | |
Polycasa Acryl® G 77 Acrylic, Injection Molding Grade Injection molding grade for record player covers, optical fibers, display windows, logos, condiment containers, desk organizers.Data was collected by ISO methods.Quinn Manufacturing Group rebranded .. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ISO value at 5mm/min. |
BASF Capron® GR15 HS 15% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron GR15 HS is a heat stabilized 15% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aest.. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ASTM D638 |
Plaskolite West Optix® CA-75 General Purpose Acrylic Resin Injection Molding and Extrusion Grade Pellets. Highest heat resistance, medium flow. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ASTM D638 |
LG Chemical Lupoy 1200-10 Polycarbonate Resin Description: LUPOY PC 1200-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ASTM D638 |
LG Chemical Lupoy 1200-15 Polycarbonate Resin Description: LUPOY PC 1200-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ASTM D638 |
LG Chemical Lupoy 1201-15 Polycarbonate Resin Description: LUPOY PC 1201-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ASTM D638 |
LG Chemical Lupoy 1301-12 Polycarbonate Resin Description: LUPOY PC 1301-12 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ASTM D638 |
LG Chemical Lupoy NF1009F 15 Polycarbonate Resin Description: LUPOY NF 1009F15, eco-friendly UL94 V0/2.0 mm, is designed for extrusion and injection molding products. It combines an excellent physical property balance of heat resistance, transpare.. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ASTM D638 |
Lucky CG-920 Acrylic May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent chemical resistance and coloring capability. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ASTM D638 |
Lucky EG-930 Acrylic, Injection Grade Injection molding grade. May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent chemical resistance and coloring capability.. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ASTM D638 |
Lucky IG-840 Acrylic, Injection Grade General purpose injection molding grade. May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent chemical resistance and col.. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ASTM D638 |
LG Chemical Lupoy 1200HP-15 Polycarbonate Resin Description: LUPOY PC 1200HP-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ASTM D638 |
LG Chemical Lupoy 1300-10 Polycarbonate Resin Description: LUPOY PC 1300-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ASTM D638 |
LG Chemical Lupoy 1300-12 Polycarbonate Resin Description: LUPOY PC 1300-12 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ASTM D638 |
LG Chemical Lupoy 1302-10 Polycarbonate Resin Description: LUPOY PC 1302-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ASTM D638 |
LG Chemical Lupoy 1303-10 Polycarbonate Resin Description: LUPOY PC 1303-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ASTM D638 |
LG Chemical Lupoy 1303AH-10 Polycarbonate Resin Description: LUPOY PC 1303AH-10 Tint Polycarbonate Resin is designed for injection molding of auto-headlamps. It exhibits an excellent physical property balance of heat resistance, transparency and .. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ASTM Data |
Styron CALIBRE™ 200 15 Polycarbonate, General Purpose CALIBRE® 200 series are general purpose, UL listed Polycarbonate resins formulated to comply with the applicable FDA and European regulations governing food contact(1). CALIBRE 200 series resins .. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ASTM D638 |
Styron CALIBREâ„¢ 201-10 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ASTM Data |
Styron CALIBRE™ 2060 15 Polycarbonate, Sterilization Grade CALIBRE® 2060 series resins are designed for those applications which use steam or ethylene oxide for sterilization. This material has excellent retention of physical properties and optical clari.. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ASTM Data |
Styron CALIBRE™ 2071 15 Polycarbonate, Sterilization Grade CALIBRE® 2071 resins are designed for those applications which use steam or ethylene oxide for sterilization while providing enhanced mold release characteristics. This material has excellent ret.. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ASTM Data |
Styron CALIBRE™ 300 10 Polycarbonate, General Purpose CALIBRE® 300 series are general purpose, UL listed polycarbonate resins. CALIBRE 300 series resins exhibit an excellent physical property balance of heat resistance, transparency and impact stren.. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ASTM D638 |
Styron CALIBREâ„¢ 301-15 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | 0.125 in, injection molded, unannealed; ASTM D638 |
Styron EMERGEâ„¢ 4310-10 Polycarbonate EMERGEâ„¢ PC 4310-10 advanced resin is high-performance polycarbonate resin offering high heat resistance and maximum toughness. Applications: Consumer Electronics and Information Technology Eq.. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | 0.125 in, injection molded, unannealed; ASTM D638 |
Styron EMERGEâ„¢ 4510-15 Polycarbonate EMERGEâ„¢ PC 4510-15 advanced resin is a general purpose polycarbonate resin offering ignition resistance, heat resistance and excellent toughness. Applications: Consumer Electronics and Inform.. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | 0.125 in, injection molded, unannealed; ASTM D638 |
Styron EMERGEâ„¢ 4530-10 Polycarbonate EMERGEâ„¢ PC 4530-10 advanced resin is a general purpose polycarbonate resin offering ignition resistance, heat resistance and excellent toughness. Applications: Consumer Electronics and Inform.. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | 0.125 in, injection molded, unannealed; ASTM D638 |
Styron EMERGEâ„¢ 4310-15 Polycarbonate EMERGEâ„¢ PC 4310-15 advanced resin is high-performance polycarbonate resin offering high heat resistance and maximum toughness. Applications: Consumer Electronics and Information Technology Eq.. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | 0.125 in, injection molded, unannealed; ASTM D638 |
Styron EMERGEâ„¢ 4530-15 Polycarbonate EMERGEâ„¢ PC 4530-15 advanced resin is a general purpose polycarbonate resin offering ultraviolet light stability, ignition resistance, heat resistance and excellent toughness. Applications: Co.. |
|||
Tensile Strength, Ultimate | 71.0 MPa @Temperature 649 °C |
10300 psi @Temperature 1200 °F |
|
AK Steel Aluminized Carbon Steel, Commercial Steel (CS Type B), Standard Grade Aluminized Type 1 coating contains approximately 91% aluminum and 9% silicon that is metallurgically bonded to the low-carbon steel substrate. May be moderately formed. A specimen cut in any direc.. |