Tensile Strength, Ultimate 29.0 - 51.0 MPa
4210 - 7400 psi
Average value: 39.7 MPa Grade Count:14
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m..
Tensile Strength, Ultimate 1.40 - 51.0 MPa

@Temperature -20.0 - 49.0 °C
203 - 7400 psi

@Temperature -4.00 - 120 °F
Average value: 19.8 MPa Grade Count:11
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate; Molded/Extruded". Each property range of values reported is minimum and maximum ..
Tensile Strength, Ultimate 14.0 - 51.0 MPa
2030 - 7400 psi
Average value: 38.4 MPa Grade Count:15
Overview of materials for PVC, Powder
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Powder". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Tensile Strength, Ultimate 0.255 - 51.0 MPa
37.0 - 7400 psi
Average value: 9.26 MPa Grade Count:573
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Elastomer, Melt-Processible Rubber". Each property range of values reported is minimum and..
Tensile Strength, Ultimate 0.150 - 51.0 MPa
21.8 - 7400 psi
Average value: 27.7 MPa Grade Count:22
Overview of materials for Polystyrene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a..
Tensile Strength, Ultimate 23.0 - 51.0 MPa

@Temperature 60.0 - 120 °C
3340 - 7400 psi

@Temperature 140 - 248 °F
Average value: 38.1 MPa Grade Count:4
Overview of materials for Polycarbonate, Molded