Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 82.7 MPa | 12000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ AS-15CF/15T Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced, PTFE Lubricated
&nb Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 82.7 - 138 MPa | 12000 - 20000 psi | Average value: 95.9 MPa Grade Count:6 |
Overview of materials for Nylon 66, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Extruded". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
Tensile Strength, Ultimate | 82.7 - 146 MPa | 12000 - 21200 psi | Average value: 114 MPa Grade Count:4 |
Overview of materials for Nylon 11 with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are includ.. |
|||
Tensile Strength, Ultimate | 82.7 MPa | 12000 psi | ASTM D638 |
Firestone C200-001 Nylon 6 Natural color. Not heat stabilized, modified, or lubricated. Chip size is 2 x 3.5 mm.Information provided by Firestone |
|||
Tensile Strength, Ultimate | 82.7 MPa @Temperature 427 °C |
12000 psi @Temperature 800 °F |
Stainless Steel (18-8) butt joint |
Lucas-Milhaupt EASY FLO Silver Based Cadmium-Bearing Filler Metal Applications: Easy-Flo is very versatile and can be used successfully on nearly all nickel, iron and copper base alloys. In certain instances, special fluxes, may be required to obtain good wettin.. |
|||
Tensile Strength, Ultimate | 82.7 MPa | 12000 psi | ASTM Data |
Styron Pulse® 759 ABS + Polycarbonate, 15% Glass Reinforced PULSE® 759 Engineering resin is a 15% glass reinforced resin designed to provide excellent processability, high heat resistance, and practical toughness. PULSE 759 Engineering resin has been used.. |
|||
Tensile Strength, Ultimate | 82.7 MPa | 12000 psi | ASTM D638 |
Techmer ES Electrafil® J-1200/CF/10 ABS, 10% Carbon Fiber Reinforced |
|||
Tensile Strength, Ultimate | 82.7 MPa | 12000 psi | ASTM Data |
Styron CALIBRE™ 5201 15 Polycarbonate, 20% Glass Reinforced CALIBRE® 5201 is a 20% glass reinforced polycarbonate resin containing mold release for optimal processing. CALIBRE 5201 resin exhibits high modulus and excellent dimensional stability.CALIBRE 52.. |
|||
Tensile Strength, Ultimate | 82.7 MPa | 12000 psi | ASTM D638 |
Applied Composites 8022 Polyester SMC Industry Application: ConstructionProduct Application: Water TreatmentDistinct Features: Ideal for Buried Applications, Construction, High Corrosion Resistance in Waste Water Treatment, Dimensional .. |
|||
Tensile Strength, Ultimate | 82.7 - 100 MPa | 12000 - 14500 psi | Average value: 91.9 MPa Grade Count:7 |
Overview of materials for Polyetherimide (PEI), Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Aramid Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Tensile Strength, Ultimate | 82.7 MPa | 12000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ PI-000/15T Polyetherimide (PEI), PTFE Lubricated
(discontinued **) Description/Features:PTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 82.7 - 124 MPa | 12000 - 18000 psi | Average value: 104 MPa Grade Count:19 |
Overview of materials for Polyphenylene Ether, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 30% Glass Filled". Specific grades with glass content between 25% and 34% are inclu.. |
|||
Tensile Strength, Ultimate | 82.7 MPa | 12000 psi | |
XXXPC Phenolic Laminate Paper based phenolic provides low cost electrical and mechanical properties. It is widely used for switchboards, panel boards, insulating washers, and intricate punched parts.Information provided b.. |