Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 689 MPa | 100000 psi | |
Pacific Sintered Materials FN-253-S(HT) 4600 Powdered Metal High performance material with high strength and wear resistance after heat treatment.Equivalent MPIF Specification: FL-4605-100HTAll information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Ultimate | 689 MPa | 100000 psi | |
Pacific Sintered Materials FX-233-T Infiltrated Alloy Steel Excellent combination of strength and shock resistance. Good for use in cams, pawls, sprockets and wear plates. Moderate tolerance control.All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Ultimate | 689 MPa | 100000 psi | |
PSM Industries Pacific Sintered Metals 4600 FN-253-S(HT) Powdered Metal High performance material with high strength and wear resistance after heat treatment Equivalent MPIF Specification: FL-4605-100HTInformation Provided by Pacific Sintered Metals, a division of PSM .. |
|||
Tensile Strength, Ultimate | 689 MPa | 100000 psi | |
PSM Industries Pacific Sintered Metals Infiltrated Alloy Steel FX-233-T Powdered Metal Excellent combination of strength and shock resistance, Good for use in cams, pawls, sprockets and wear plates, Moderate tolerance controlInformation Provided by Pacific Sintered Metals, a division .. |
|||
Tensile Strength, Ultimate | 689 MPa | 99900 psi | |
Materion BrushBronze® 630 (AMS 4640) 3.0" - 5.0" Information supplied by Brush Wellman Engineered Materials.BrushBronze™ 630 is an Aluminum-Nickel-Bronze alloy that combines high strength along with resistance to wear under severe loading con.. |
|||
Tensile Strength, Ultimate | 689 - 724 MPa | 100000 - 105000 psi | |
Materion BrushCAST® 20C High Strength Casting Alloy (As Cast & Aged) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Tensile Strength, Ultimate | 689 - 724 MPa | 100000 - 105000 psi | |
Materion BrushCAST® 21C High Strength Casting Alloy (As Cast & Aged) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Tensile Strength, Ultimate | 689 - 724 MPa | 100000 - 105000 psi | |
Materion BrushCAST® 20CT Fine Grain Casting Alloy (As Cast & Aged) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Tensile Strength, Ultimate | 689 MPa | 100000 psi | |
Meehanite Almanite® WSH Wear and Abrasion Resisting Cast Iron Type WSH is an austenitic nodular iron possessing superior tensile strength, toughness and ability to work harden under conditions of severe pounding impact. It is extremely difficult to machine. .. |
|||
Tensile Strength, Ultimate | 689 - 1170 MPa | 100000 - 170000 psi | |
Meehanite Ductliron® SH-100 Nodular Graphite Ductile Iron Type SP-100 is characterized by its exceptional hardenability. It is particularly suited where high strengths are desired in relatively heavy casting sections. In the as-cast condition it has a pe.. |
|||
Tensile Strength, Ultimate | 689 - 827 MPa | 100000 - 120000 psi | |
Meehanite HSV Heat Resisting Cast Iron Type HSV is an iron developed essentially for engineering parts subjected to long continuous heating. It has been designed to have the maximum load bearing ability.General Meehanite information - M.. |
|||
Tensile Strength, Ultimate | 689 - 1030 MPa | 100000 - 150000 psi | |
Special Metals DURANICKEL® 301 (UNS N03301) Cold-Drawn Rod and Bar Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Cold-Drawn Rod and Bar specifically. Other property values are typical of annealed DURANICKEL®.. |
|||
Tensile Strength, Ultimate | 689 MPa | 100000 psi | |
Special Metals INCOLOY® 25-6M0 Super Austenitic Stainless Steel (UNS N08926) Data provided by the manufacturer, Special Metals. |
|||
Tensile Strength, Ultimate | 689 MPa | 100000 psi | |
Special Metals INCONEL® 690 Nickel Superalloy, Hot Rolled Flat, 2.0 inch (51 mm) Diameter Composition adjustments for nuclear applications: 28-31 Cr; 0.04 max C; 0.10 max Co.Tensile strength (ultimate and yield) and elongation values reported here are typical for Hot Rolled Flat, 2.0 inc.. |
|||
Tensile Strength, Ultimate | 689 MPa | 100000 psi | |
Universal Wire Works C-276 Nickel Alloy Welding Wire Alloy C-276 is a low carbon, nickel base alloy containing significant amounts of molybdenum and chromium. Alloy C-276 is one of the most universally corrosion resistant alloys available. This alloy .. |
|||
Tensile Strength, Ultimate | >= 689 MPa | >= 100000 psi | |
Universal Wire Works Inconel 625 (AMS 5837) Filler Metal Inconel Filler Metal 625 is recommended for gas metal arc and gas tungsten arc welding of nickel base alloys 625 and 601, Incoloy alloys, carbon steels, low alloy steels and stainless steels. This a.. |
|||
Tensile Strength, Ultimate | 689 - 786 MPa | 100000 - 114000 psi | |
Eagle Brass 510 Phosphor Bronzes 5% A, Extra Spring Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info.. |
|||
Tensile Strength, Ultimate | 689 MPa | 100000 psi | |
ECOMold 135 Copper Mold Material ECOMold® copper alloys (beryllium-free) are engineered specifically for plastics industry applications. ECOMold® 135 has superior thermal conductivity compared to other common mold materials. T.. |
|||
Tensile Strength, Ultimate | 689 MPa | 99900 psi | Forgings |
CMW® 100 Copper Alloy CMW® 100 material is a heat treatable, high strength, high conductivity copper base alloy. Its properties are a combination of highest strength and hardness with relatively high electrical and ther.. |
|||
Tensile Strength, Ultimate | 689 MPa | 100000 psi | annealed |
CMW® ELKONIUM 32 platinum based alloy Platinum has complete freedom from atmospheric corrosion and is preferred for devices that have low closed forces and where surety of making a circuit may be a problem. It has a high melting point (.. |
|||
Tensile Strength, Ultimate | 689 MPa | 100000 psi | cold worked |
CMW® ELKONIUM 405 palladium based alloy Palladium belongs to the platinum group of metals and like platinum is highly resistant to atmospheric corrosion; however, it begins to tarnish at temperatures above 400(C. It has a high melting poi.. |
|||
Tensile Strength, Ultimate | 689 MPa | 100000 psi | cold worked |
CMW® ELKONIUM 41 palladium based alloy Palladium belongs to the platinum group of metals and like platinum is highly resistant to atmospheric corrosion; however, it begins to tarnish at temperatures above 400(C. It has a high melting poi.. |
|||
Tensile Strength, Ultimate | 689 MPa | 100000 psi | cold worked |
CMW® ELKONIUM 42 palladium based alloy Palladium belongs to the platinum group of metals and like platinum is highly resistant to atmospheric corrosion; however, it begins to tarnish at temperatures above 400(C. It has a high melting poi.. |
|||
Tensile Strength, Ultimate | 689 - 993 MPa | 99900 - 144000 psi | Typical, (Gauge, 0.028" -0.084") |
AK Steel NITRONIC® 19-D Duplex Stainless Steel AK Steel NITRONIC® 19D is a stainless steel with a mixed ferrite and austenite structure. This alloy provides high yield strength (65 ksi minimum {448 MPa}),
good drawing and welding characteristi.. |
|||
Tensile Strength, Ultimate | 689 MPa @Thickness 1.63 mm |
99900 psi @Thickness 0.0640 in |
Annealed at 2050°F, Longitudinal |
AK Steel NITRONIC® 30 Austenitic Stainless Steel AK Steel NITRONIC 30 Stainless Steel offers significantly higher strength than Type 304 and potential for applications requiring good resistance to aqueous and atmospheric corrosion resistance combi.. |
|||
Tensile Strength, Ultimate | >= 689 MPa | >= 99900 psi | Hardened and Tempered |
ATI Allegheny Ludlum AL 403™ Martensitic Stainless Steel Characteristics: corrosion resistant, heat resistant, oxidation resistant up to 1400°F.Information provided by Allegheny Ludlum |
|||
Tensile Strength, Ultimate | 689 - 827 MPa | 99900 - 120000 psi | |
Ametek AM 388™ Alloy (UNS C72650) TM00 Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |