Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Materion BrushBronze® 630 (AMS 4640) 3.0" - 5.0"

Category Metal , Nonferrous Metal , Copper Alloy , Bronze , Copper Casting Alloy
Manufacturer Materion Corporation (former Brush Wellman)
Trade Name BrushBronze®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Materion BrushBronze® 630 (AMS 4640) 3.0" - 5.0".pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information supplied by Brush Wellman Engineered Materials.BrushBronzeâ„¢ 630 is an Aluminum-Nickel-Bronze alloy that combines high strength along with resistance to wear under severe loading conditions. This material, specified as AMS 4640, is frequently used for very demanding aerospace applications, including, but not limited to: bushings, spherical and rod end bearings, rub pads, and wear strips. This material is also commonly used for applications in the oil and gas and other durable goods markets.BrushBronzeâ„¢ 630 (AMS 4640) offers several significant advantages over other materials available in the marketplace due to the EquaCastâ„¢ process:Higher and more consistent mechanical propertiesImproved service lifeEase of useBrush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.
Mechanical Properties Metric English Comments
Hardness, Brinell 187 - 241
187 - 241
Tensile Strength, Ultimate 689 MPa
99900 psi
Tensile Strength, Yield 345 MPa
50000 psi
Elongation at Break 10 %
10 %
Component Elements Properties Metric English Comments
Aluminum, Al 9.0 - 11 %
9.0 - 11 %
Copper, Cu >= 78 %
>= 78 %
Iron, Fe 2.0 - 4.0 %
2.0 - 4.0 %
Manganese, Mn <= 1.5 %
<= 1.5 %
Nickel, Ni 4.0 - 5.5 %
4.0 - 5.5 %
Silicon, Si <= 0.25 %
<= 0.25 %
Tin, Sn <= 0.20 %
<= 0.20 %
Zinc, Zn <= 0.30 %
<= 0.30 %
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved