Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 6.55 MPa | 950 psi | Original Properties; ASTM D412 Die C |
Freudenberg Simrit S50 Silicone Elastomer (VMQ) General Purpose; AMS 3301; A-A-59588 (ZZ-R-765) Class 2A, 2B Grade 40; Good heat resistance. Poor resistance to abrasion, tear and cut growth; low tensile strength; inferior resistance to oil, gasol.. |
|||
Tensile Strength, Ultimate | 6.55 MPa | 950 psi | Original Properties; ASTM D412 Die C |
Freudenberg Simrit S60 Silicone Elastomer (VMQ) General Purpose; AMS 3301; A-A-59588 (ZZ-R-765) Class 2A, 2B Grade 40; Good heat resistance. Poor resistance to abrasion, tear and cut growth; low tensile strength; inferior resistance to oil, gasol.. |
|||
Tensile Strength, Ultimate | 6.55 MPa | 950 psi | |
Sylvin Technologies 8999-60 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 6.55 MPa | 950 psi | |
Sylvin Technologies 9999-60 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 6.55 MPa | 950 psi | |
Colorite Polymers Flexchem 4051-02 Vinyl Compound Description: The Flexchem "51" series is a group of translucent, flexible, non-toxic vinyl compounds which were specifically developed to replace silicone in various applications. These compounds ut.. |
|||
Tensile Strength, Ultimate | 6.55 MPa | 950 psi | After 7 days at 257°F (125°C); ASTM D573; ISO 188 |
Advanced Polymer Alloys Alcryn® 2060 NC Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Tensile Strength, Ultimate | 6.55 MPa | 950 psi | ASTM D638 |
Colorite Polymers 4543 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Tensile Strength, Ultimate | 6.55 MPa | 950 psi | ASTM D412 |
Arlon R3792-920-10R##-P0 Silicone Rubber This self-fusible silicone tape is specially formulated to yield improved flexibility, elongation and elastic recovery at low operating temperature (-70°C to -100°C) where standard fusible silicon.. |