Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 586 MPa | 85000 psi | |
Hogen Duralloy H20TC 70 Tungsten Carbide/30 Copper PM Metal Composite Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Extremely hard and wear resistant t.. |
|||
Tensile Strength, Ultimate | 586 MPa | 85000 psi | |
Hogen Duralloy H5W 70 Tungsten/30 Copper PM Metal Composite RWMA Class 10.Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 10 material is .. |
|||
Tensile Strength, Ultimate | 586 - 621 MPa | 85000 - 90000 psi | |
Materion BrushCAST® 275CT Fine Grain Casting Alloy (As Cast) Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri.. |
|||
Tensile Strength, Ultimate | 586 MPa | 85000 psi | |
Mi-Tech Metals CW70 70 Tungsten/30 Copper PM Metal Composite RWMA Class 10.Mi-Tech refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 10 material is recomme.. |
|||
Tensile Strength, Ultimate | 586 MPa @Temperature 649 °C |
85000 psi @Temperature 1200 °F |
|
Haynes Hastelloy® C-22® alloy, 0.71-3.2 mm thick sheet, solution heat treated HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Tensile Strength, Ultimate | 586 - 689 MPa | 85000 - 100000 psi | Annealed temper |
Special Metals INCONEL® 601GC® Nickel Superalloy Data provided by the manufacturer, Special Metals. |
|||
Tensile Strength, Ultimate | 586 MPa | 85000 psi | |
Universal Wire Works 310 Stainless Steel (AMS 5694) Filler Metal Universal 310 alloy is primarily used for welding type 310 stainless steels, dissimilar steels and such types as 405, 410 and 430 steels when preheat and postheat are not practical. This alloy exhib.. |
|||
Tensile Strength, Ultimate | 586 - 641 MPa | 85000 - 93000 psi | |
Eagle Brass 240 Low Brass, Spring CDA 240 has excellent ductility, corrosion resistance and strength which allows it to be deep drawn, etched, stamped, blanked and bent. Typical uses include musical instruments, battery caps, flexib.. |
|||
Tensile Strength, Ultimate | 586 - 689 MPa | 85000 - 100000 psi | |
Eagle Brass 521 Phosphor Bronzes 8% C, Hard Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical.. |
|||
Tensile Strength, Ultimate | 586 - 689 MPa | 85000 - 100000 psi | |
Eagle Brass 725 Copper Nickel Tin, Spring Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
Tensile Strength, Ultimate | 586 MPa | 85000 psi | |
Crucible Steel 321 Chromium-Nickel Steel Crucible 321 is a non-hardenable, low carbon austenitic chromium-nickel steel which is particularly adaptable for parts fabricated by welding without postweld annealing for use at temperatures betwe.. |
|||
Tensile Strength, Ultimate | 586 MPa | 85000 psi | |
CMW® ELKALOY D120 Copper Alloy, Aluminum Bronze ELKALOY® D alloys are aluminum bronze type casting alloys. The sequence, ELKALOY® D, D110, D120, D130 materials represents increasing hardness and abrasion resistance but reduced electrical and th.. |
|||
Tensile Strength, Ultimate | 586 MPa | 85000 psi | |
CMW® ELKALOY D130 Copper Alloy, Aluminum Bronze ELKALOY® D alloys are aluminum bronze type casting alloys. The sequence, ELKALOY® D, D110, D120, D130 materials represents increasing hardness and abrasion resistance but reduced electrical and th.. |
|||
Tensile Strength, Ultimate | 586 MPa | 85000 psi | Typical |
Dura-Bar 80-55-06 Continuously Cast Ductile Iron Bar Stock ASTM A536 Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as a direct replacement for.. |
|||
Tensile Strength, Ultimate | 586 MPa | 85000 psi | |
AK Steel 304L Austenitic Stainless steel AK Steel 304L is an extra low-carbon variation of Type 304, that eliminates carbide precipitation due to welding. AK Steel 304L can be used in the "as-welded" condition, even in severe corrosive co.. |
|||
Tensile Strength, Ultimate | 586 MPa | 85000 psi | Annealed |
AK Steel 305 Austenitic Stainless steel AK Steel 305 can be spun and deep drawn more easily due to an increased nickel content that decreases work hardening. It is non-magnetic and cannot be hardened by heat treatment. Typical uses incl.. |
|||
Tensile Strength, Ultimate | 586 MPa | 85000 psi | Annealed |
AK Steel 420 Martensitic Stainless steel AK Steel 420 provides corrosion resistance similar to Type 410 martensitic stainless steel plus increased strength and hardness. It is magnetic in both the annealed and hardened conditions. Maximu.. |
|||
Tensile Strength, Ultimate | 586 MPa | 85000 psi | Annealed |
AK Steel 420 ULTRA HONE® Martensitic Stainless steel AK Steel 420 provides corrosion resistance similar to Type 410 martensitic stainless steel plus increased strength and hardness. It is magnetic in both the annealed and hardened conditions. Maximu.. |
|||
Tensile Strength, Ultimate | 586 MPa | 85000 psi | Annealed |
AK Steel 420HC Martensitic Stainless steel AK Steel 420 provides corrosion resistance similar to Type 410 martensitic stainless steel plus increased strength and hardness. It is magnetic in both the annealed and hardened conditions. Maximu.. |
|||
Tensile Strength, Ultimate | 586 MPa | 85000 psi | |
Carpenter BioDur™ 316LS Stainless Medical Implant Alloy, Annealed Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Vacuum arc remelted (VAR), low carbon version of Type 316 stainless. The secondary premium melting step (VAR) imparts impro.. |
|||
Tensile Strength, Ultimate | 586 - 655 MPa | 85000 - 95000 psi | |
Ametek AM 388™ Alloy (UNS C72650) TD04 Hard Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |
|||
Tensile Strength, Ultimate | 586 - 589 MPa | 85000 - 85400 psi | |
Ametek High Purity Nickel Strip 899A Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Ultimate | 586 - 589 MPa | 85000 - 85400 psi | |
Ametek High Purity Nickel Strip 899L Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Ultimate | 586 MPa | 85000 psi | |
ATI Allvac® Nickelvac® 800 & 800-H UNS N08800 & UNS N08810 Nickel Superalloy Corrosion-resistant alloy for petrochemical and food processing equipment, tubing, heat exchangers, and furnaces.Property values are for samples in the metallurgical condition: 2100°F anneal + wate.. |
|||
Tensile Strength, Ultimate | 586 MPa @Temperature 260 °C |
85000 psi @Temperature 500 °F |
|
ATI Allegheny Ludlum AL 2003™ Duplex Stainless Steel Characteristics: superior stress corrosion cracking resistance to Types 316 and 317, yield strength double that of conventional austenitic stainless steel, good corrosion resistance, good chloride s.. |
|||
Tensile Strength, Ultimate | 586 - 589 MPa | 85000 - 85400 psi | |
Ametek High Purity Nickel Strip 899M Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |