Material Notes:
Corrosion-resistant alloy for petrochemical and food processing equipment, tubing, heat exchangers, and furnaces.Property values are for samples in the metallurgical condition: 2100°F anneal + water quench.Information provided by Allvac, An Allegheny Teledyne Company.
Physical Properties Metric English Comments
Density 7.94 g/cc
0.287 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 72
72
Tensile Strength, Ultimate 586 MPa
85000 psi
Tensile Strength, Yield 262 MPa

@Strain 0.200 %
38000 psi

@Strain 0.200 %
Elongation at Break 50 %
50 %
Reduction of Area 76 %
76 %
Component Elements Properties Metric English Comments
Aluminum, Al 0.37 %
0.37 %
Carbon, C 0.050 %
0.050 %
Chromium, Cr 21 %
21 %
Copper, Cu 0.37 %
0.37 %
Iron, Fe 44 %
44 %
as balance
Manganese, Mn 0.75 %
0.75 %
Nickel, Ni 32.5 %
32.5 %
Silicon, Si 0.50 %
0.50 %
Sulfur, S 0.0070 %
0.0070 %
Titanium, Ti 0.37 %
0.37 %