Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 29.4 MPa | 4260 psi | ASTM D638-95 |
Multibase Multi-Pro® 1010 C Natural 10% Filler Content Polypropylene Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 29.4 MPa | 4270 psi | ISO 527 |
Polikim Polypropylene Polypropylene is an olefin class plastic with low density. It has good chemical and electrical properties and is rigid. Its use under 0°C is not recommended as its mechanical properties weaken. Nor.. |
|||
Tensile Strength, Ultimate | 29.4 MPa | 4270 psi | ASTM D638 |
Global MB-6366 High Density Polyethylene Description-high density for high quality, excellent creep & chemical resistanceApplications-drinking water pipe, industrial pipe, sewer pipeInformation provided by Global Polymers Corporation. |
|||
Tensile Strength, Ultimate | 29.4 MPa | 4270 psi | ASTM D638 |
KKPC Kuhmo HI 425TV High Flow/High Heat Resistant HIPS Key features: High-impact, High heat resistance. Common Uses: TV cabinets , phonograph housings, humidifiers, typewriter bodies, sporting goods, office appliance housings.HIPS is a functional resin .. |
|||
Tensile Strength, Ultimate | 29.4 MPa | 4270 psi | 150°C, 40 min., Pressure Vulcanization. -3% Change after 100°C, 70 hrs, Oil Immersion |
KKPC KOSYN KNB 230 Acrylonitrile Butadiene Rubber (NBR) Acrylonitrile Butadiene Rubber (NBR)Characteristics: KOSYN KNB is copolymer of high oil resistance and chemical resistance made from acrylonitrile and butadiene by the cold emulsion polymerization. .. |
|||
Tensile Strength, Ultimate | 29.4 MPa | 4270 psi | 150°C, 40 min., Pressure Vulcanization. -8% Change after 100°C, 70 hrs, Oil Immersion |
KKPC KOSYN KNB 35LL Acrylonitrile Butadiene Rubber (NBR) Acrylonitrile Butadiene Rubber (NBR)Characteristics: KOSYN KNB is copolymer of high oil resistance and chemical resistance made from acrylonitrile and butadiene by the cold emulsion polymerization. .. |
|||
Tensile Strength, Ultimate | 29.4 MPa | 4270 psi | 150°C, 40 min., Pressure Vulcanization. -1% Change after 100°C, 70 hrs, Oil Immersion |
KKPC KOSYN KNB 40H Acrylonitrile Butadiene Rubber (NBR) Acrylonitrile Butadiene Rubber (NBR)Characteristics: KOSYN KNB is copolymer of high oil resistance and chemical resistance made from acrylonitrile and butadiene by the cold emulsion polymerization. .. |
|||
Tensile Strength, Ultimate | 29.4 MPa | 4270 psi | |
Shinil Chemical SHINCON PMMA Electro Conductive Polymer SHINCON is the product line of SHINIL's electrically conductive compound which is able to dissipate the electrostatic charge (ESD) effectively. Shinil has developed SHINCON products using Shinil's .. |
|||
Tensile Strength, Ultimate | 29.4 MPa | 4270 psi | |
Shinil Chemical SHINSTAT ABS Electrostatic Control Polymer Injection Grade SHINSTAT is an Inherently Dissipative Polymer (IDP) compound which can discharge the electrostatic charge (ESD) effectively. Shinil has designed SHINSTAT using Shinil's patented IDP technology for .. |
|||
Tensile Strength, Ultimate | 29.4 MPa | 4270 psi | |
Shinil Chemical SHINSTAT PETG Electrostatic Control Polymer Sheet Grade SHINSTAT is an Inherently Dissipative Polymer (IDP) compound which can discharge the electrostatic charge (ESD) effectively. Shinil has designed SHINSTAT using Shinil's patented IDP technology for .. |
|||
Tensile Strength, Ultimate | 29.4 MPa | 4270 psi | |
Shinil Chemical SHINSTAT PP Electrostatic Control Polymer Sheet Grade SHINSTAT is an Inherently Dissipative Polymer (IDP) compound which can discharge the electrostatic charge (ESD) effectively. Shinil has designed SHINSTAT using Shinil's patented IDP technology for .. |
|||
Tensile Strength, Ultimate | 29.4 MPa | 4270 psi | |
Shinil Chemical SHINSTRA PA-66 Devlop Structural Polymer Window Strip SHINSTRA is the product line of structural polymer compound which exhibits excellent physical, mechanical, and thermal properties. Shinil uses the state-of-the-art dispersion and blending technolog.. |
|||
Tensile Strength, Ultimate | 29.4 MPa | 4270 psi | ASTM D792, Die C |
Stellarchem SE/PA745B TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Tensile Strength, Ultimate | 29.4 MPa | 4270 psi | ASTM D412 |
SK Chemicals SKYTHANE® CR180A Calendaring Series, Polyether Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Tensile Strength, Ultimate | 29.4 MPa | 4270 psi | ASTM D412 |
SK Chemicals SKYTHANE® R180A C series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tensile Strength, Ultimate | 29.4 MPa | 4270 psi | ASTM D412 |
SK Chemicals SKYTHANE® R180A Polyether Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Tensile Strength, Ultimate | 29.4 MPa | 4270 psi | ASTM D638 |
SK Chemicals SKYTHANE® US230 Magnetic Binder Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Tensile Strength, Ultimate | 29.4 MPa | 4270 psi | ASTM D412 |
SK Chemicals SKYTHANE® 180A R series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tensile Strength, Ultimate | 29.4 MPa | 4270 psi | ASTM D412 |
Lubrizol Estane® X-585A-31 Thermoplastic Polyurethane Type: Estane® X585A-31 is a Shore 95A, polyester grade without lubricant thermoplastic polyurethane (TPU). USP Class VI Certified.Uses: Extrusion, Film Blowing.Information Provided by The Lubrizol.. |
|||
Tensile Strength, Ultimate | 29.4 MPa | 4270 psi | ASTM D412 |
Lubrizol Estane® CS185A Thermoplastic Polyurethane Type: Estane® CS185A is a Shore 85A, polyester grade, calendering processible thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Calendering, Molt roll processing.Inf.. |
|||
Tensile Strength, Ultimate | 29.4 MPa | 4270 psi | ASTM D412 |
Lubrizol Estane® R175A Thermoplastic Polyurethane Type: Estane® R175A is a Shore 75A, plasticized grade thermoplastic polyurethane (TPU).Uses: Injection Molding.Information Provided by The Lubrizol Corporation |
|||
Tensile Strength, Ultimate | 29.4 MPa | 4270 psi | ASTM D412 |
Lubrizol Estane® S175A Thermoplastic Polyurethane Type: Estane® S175A is a Shore 77A, polyester type thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion.Availability: Americas, Europe, Mid.. |