Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 17.9 MPa | 2600 psi | 20" / min.; ASTM D-683-95 |
Multibase Multi-Flex® TPO D 5305 Multi-Flex® D 5303 is a TOP compound for automotive applications such as bumper covers and side panels.Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 17.9 - 60.7 MPa | 2600 - 8800 psi | Average value: 40.2 MPa Grade Count:86 |
Overview of materials for Polystyrene, Molded, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Tensile Strength, Ultimate | 17.9 MPa | 2600 psi | ASTM D882 |
M. Holland Company LD219AA LDPE
(discontinued **) Features: Good Processability, Ultra High ToughnessUses: Bottles, PackagingProcessing Method: Blow MoldingInformation provided by M. Holland. |
|||
Tensile Strength, Ultimate | 17.9 MPa | 2600 psi | |
Freudenberg Simrit Viton® SC1106 CV75 ETP Excellent resistance to most chemicals. The performance of these products is greater than traditional fluoroelastomers. Avoid use in strong bases or amines. Typical used in wet etch, dry etch, CVD, .. |
|||
Tensile Strength, Ultimate | 17.9 MPa | 2600 psi | |
Freudenberg Simrit Viton® SC1106 CV75 HP-1 (TFE/P) The lowest elemental extractable fluoroelastomer available. Is based on an acid-resistant fluoroelastomer. Typical used as a coater/ developer, dry etch, wet etch, cleaning, resists stripping, ion i.. |
|||
Tensile Strength, Ultimate | 17.9 MPa | 2600 psi | |
Sylvin Technologies 8600-80 Clear PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 17.9 MPa | 2600 psi | |
Sylvin Technologies 8925-85 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 17.9 MPa | 2600 psi | |
Sylvin Technologies 8940-90 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 17.9 MPa | 2600 psi | |
Sylvin Technologies 9925-85 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 17.9 MPa | 2600 psi | X-Direction; ASTM D638 |
SpinTech Veritexâ„¢ Shape Memory Polymer Composite Veritexâ„¢ is a fiber-reinforced composite that uses a shape memory polymer, VeriflexÂ, as the matrix. This allows Veritex to easily change shape above its activation temperature. At lower tempe.. |
|||
Tensile Strength, Ultimate | 17.9 MPa | 2600 psi | |
Sylvin Technologies 6128-90 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 17.9 MPa | 2600 psi | ASTM D638 |
Dow AMPLIFY™ EA 100 Ethylene-ethyl Acrylate (EEA) AMPLIFY™ EA 100 Functional Polymer is produced via a high pressure reactor. It exhibits high flexibility and imparts low temperature toughness to a wide range of engineering resins. This polymer.. |
|||
Tensile Strength, Ultimate | 17.9 MPa | 2600 psi | |
DuPont Performance Polymers Kalrez® 7075 FFKM Perfluoroelastomer Kalrez® Spectrum™ 7075 is designed specifically for the needs of the chemical processing industry. Compound 7075 broadens the family of Spectrum™ sealing options with a compound that has enhanced.. |
|||
Tensile Strength, Ultimate | 17.9 MPa | 2600 psi | ASTM D412 |
Dow Tyrin® CM0730 Formulation FormulationTyrin® CPE Elastomer |
|||
Tensile Strength, Ultimate | 17.9 MPa | 2600 psi | ASTM D412 |
Colorite Polymers CS9040UL Wire and Cable Jacket Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Tensile Strength, Ultimate | 17.9 MPa | 2600 psi | ASTM Data |
Dow Retain® PS-4000 Polystyrene Data provided by Dow Chemical. |
|||
Tensile Strength, Ultimate | 17.9 MPa | 2600 psi | ASTM D638 |
Colorite Polymers 7342 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Tensile Strength, Ultimate | 17.9 MPa | 2600 psi | ASTM D638 |
Colorite Polymers 8077 Non-Phthalate 77 Series Vinyl Compound Description: The Colorite 77 series is a family of compounds designed for those medical device producers that require the use of a non-phthalate plasticizer that has superior resistance to extractio.. |
|||
Tensile Strength, Ultimate | 17.9 MPa | 2600 psi | ASTM D638 |
Colorite Polymers 8088 Non-Phthalate 88 Series Vinyl Compound Description: The Colorite 88 series is a family of vinyl non-toxic compounds formulated to provide excellent low temperature flexibility characteristics. These compounds are designed for outside doo.. |
|||
Tensile Strength, Ultimate | 17.9 MPa | 2600 psi | ASTM D412 |
Colorite Polymers CS6033UL Wire and Cable Insulation Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Tensile Strength, Ultimate | 17.9 MPa | 2600 psi | ASTM D412 |
Colorite Polymers CS7559LS Wire and Cable Insulation Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Tensile Strength, Ultimate | 17.9 MPa | 2600 psi | |
Dymax 3095 Solvent-Free Plastic Adhesive Solvent-Free Adhesives for Plastic Assembly in SecondsDymax® Light-Weld® and Ultra 3000 Series UV and UV/Visible Curing Adhesives for plastic assembly provide instant durable bonds to cure a wide .. |
|||
Tensile Strength, Ultimate | 17.9 MPa | 2600 psi | |
Dymax 9-20275 Coil Terminating, Tamper proofing and Structural Electronic Bonder High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 9-20275 Coil Terminating, Tamper proofing and Structural Electronic BonderExcellent adhesion to plastics, glass, met.. |
|||
Tensile Strength, Ultimate | 17.9 MPa | 2600 psi | ASTM D638 |
Buckeye Polymers BP Flex D5606 TPO TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment. These resins have excellent UV resistance and have a.. |
|||
Tensile Strength, Ultimate | 17.9 MPa @Temperature 1090 °C |
2600 psi @Temperature 2000 °F |
Transverse |
AK Steel NITRONIC® 19-D Duplex Stainless Steel AK Steel NITRONIC® 19D is a stainless steel with a mixed ferrite and austenite structure. This alloy provides high yield strength (65 ksi minimum {448 MPa}),
good drawing and welding characteristi.. |
|||
Tensile Strength, Ultimate | 17.9 MPa | 2590 psi | ASTM D638 |
Colorite Polymers 7777 Non-Phthalate 77 Series Vinyl Compound Description: The Colorite 77 series is a family of compounds designed for those medical device producers that require the use of a non-phthalate plasticizer that has superior resistance to extractio.. |
|||
Tensile Strength, Ultimate | 17.9 MPa | 2600 psi | ASTM D638 |
Colorite Polymers 7900FR General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Tensile Strength, Ultimate | 17.9 MPa | 2600 psi | |
Dymax 9-3095-Gel Strain Relief, Wire and Parts Tacking Adhesive High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 9-3095-Gel Strain Relief, Wire and Parts Tacking AdhesiveFor fastest curing, cure with UV and visible light Cure Typ.. |