Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 165 MPa | 24000 psi | ASTM D638 |
Nylene® 9110 G43 , 43% Glass Reinforced Nylon 6/10 Description: Nylene® 9110 G43 is a 43% glass fiber reinforced specialty nylon. |
|||
Tensile Strength, Ultimate | 165 MPa | 23900 psi | ASTM D638 |
Solvay Specialty Polymers Ryton® R-4-230BL Polyphenylene Sulfide Compound
(Unverified Data**) Black Polyphenylene Sulfide CompoundRyton® R-4-230BL is an advanced 40% fiberglass reinforced polyphenylene sulfide compound which provides reduced flash and improved processability compared to oth.. |
|||
Tensile Strength, Ultimate | 165 MPa | 24000 psi | ASTM D638 |
Global GPEI-230 30% Glass Filled Reinforced Polyetherimide Alloy Information provided by Global Polymers Corporation. |
|||
Tensile Strength, Ultimate | >= 165 MPa | >= 23900 psi | |
MetalTek Bearium® B-8 Bearing Bronze Exceptional frictional properties as a result of uniformly dispersed microstructure constituents.Applications: Turbine thrust bearings, centrifuge bushings, shaft sleeves, and other severe duty, mis.. |
|||
Tensile Strength, Ultimate | 165 MPa | 24000 psi | ASTM D638 |
Techmer ES Plaslube® J-3/30/TF/13/SI/2 Nylon 6, 30% GFR, 13% PTFE, 2% Silicone Plaslube glass fiber reinforced polytetrafluoroethylene (PTFE) lubricated nylon 612 grades offer a unique balance of excellent wear and friction performance with good dimensional stability and mecha.. |
|||
Tensile Strength, Ultimate | 165 MPa | 23900 psi | |
Alcoa MIC-6 Aluminum Mold Alloy MIC-6 is a blend of the most desirable features of many individual metals. The result is a cast aluminum plate that meets the challenge of product accuracy demanded by today’s industry.Because of i.. |
|||
Tensile Strength, Ultimate | 165 MPa | 23900 psi | Annealed |
CMW® D505F Silver Nickel Contact Material For electrical contacts.Information provided by CMW Inc. |
|||
Tensile Strength, Ultimate | 165 MPa | 23900 psi | Rm |
ALIMEX ACP 6000 Aluminum Cast Plate Aluminum cast plate ACP 6000 is a 7xxx series alloy surface-machined plate. This type of alloy ensures excellent machinability characteristics and adequate tensile strength. Thickness, flatness and .. |
|||
Tensile Strength, Ultimate | 165 MPa | 24000 psi | Lengthwise; ASTM D638 |
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 3/16" to 1/4" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Tensile Strength, Ultimate | 165 MPa | 23900 psi | ASTM D638 |
Chem Polymer Chemlon 233 G Nylon 6, 33% Glass Fiber Reinforced A 33% glass fiber reinforced nylon 6 offering excellent high temperature performance, dimensional stability, tensile strength and impact resistance.Data provided by the manufacturer, Chem Polymer. |
|||
Tensile Strength, Ultimate | 165 MPa | 24000 psi | |
AIM 35.7Sn/35.7Pb/28.6Bi Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |
|||
Tensile Strength, Ultimate | 165 MPa | 24000 psi | Lengthwise; ASTM D638 |
Bedford Plastics Glass Reinforced Polyester Flat Sheet 1/8" Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |
|||
Tensile Strength, Ultimate | 165 MPa | 24000 psi | Lengthwise; ASTM D638 |
Bedford Plastics Glass Reinforced Polyester Flat Sheet, 3/8" to 1" Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |
|||
Tensile Strength, Ultimate | 165 MPa | 23900 psi | ASTM D638 |
A. Schulman ComAlloy Hiloy® 518 Polycarbonate, Carbon Fiber Reinforced Data provided by the manufacturer, ComAlloy International Company.40% Carbon Fiber Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Ultimate | 165 MPa | 23900 psi | ASTM D638 |
A. Schulman ComAlloy Lubrilon® 646 Nylon 6/12, Carbon Fiber/PTFE Reinforced Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Tensile Strength, Ultimate | 165 MPa | 23900 psi | ISO 527-1/-2 |
DSM Arnite® TV4 491 (PBT+PET)-GF50 |
|||
Tensile Strength, Ultimate | 165 MPa | 23900 psi | ASTM D638 |
Chevron Phillips Xtel® XK2140 Polyphenylene Sulfide Alloy
(discontinued **) Black Polyphenylene Sulfide AlloyXtel™ XK2140 is a high performance, glass fiber reinforced, PPS-based alloy developed to provide excellent mechanical strength and electrical properties along with .. |