Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 15.0 MPa | 2180 psi | |
3M Dyneon™ Fluorel™ FE-5620Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c.. |
|||
Tensile Strength, Ultimate | 15.0 MPa | 2180 psi | |
3M Dyneon™ Fluorel™ FC-2176 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Good general purpose grade with good .. |
|||
Tensile Strength, Ultimate | 15.0 MPa | 2180 psi | |
3M Dyneon™ Fluorel™ FLS-2530 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 69%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. High fluorine dipolymer with improved f.. |
|||
Tensile Strength, Ultimate | 15.0 MPa | 2180 psi | |
3M Dyneon™ Fluorel™ FC-2120 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Dipolymer for difficult extrusions. .. |
|||
Tensile Strength, Ultimate | 15.0 MPa | 2180 psi | |
3M Dyneon™ Fluorel™ FC-2182 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Dipolymer for autoclave curing. Used.. |
|||
Tensile Strength, Ultimate | 15.0 MPa | 2180 psi | |
3M Dyneon™ Fluorel™ FT-2350 Fluoroelastomer VF2 + HFP + TFE Terpolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 68.6%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Improved retention of elongation afte.. |
|||
Tensile Strength, Ultimate | 15.0 - 195 MPa @Temperature -40.0 - 150 °C |
2180 - 28300 psi @Temperature -40.0 - 302 °F |
Average value: 93.9 MPa Grade Count:11 |
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25.. |
|||
Tensile Strength, Ultimate | 15.0 MPa | 2180 psi | ASTM D638 |
North Wood Plastics HDPE with 60% Wood Fiber Data provided by North Wood Plastics, Inc. |
|||
Tensile Strength, Ultimate | 15.0 - 110 MPa @Temperature 60.0 - 150 °C |
2180 - 16000 psi @Temperature 140 - 302 °F |
Average value: 58.4 MPa Grade Count:4 |
Overview of materials for Nylon 12 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en.. |
|||
Tensile Strength, Ultimate | 15.0 MPa | 2180 psi | at max load; ISO 527 |
A. Schulman FORMION™ FI 330 Ionomer Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 15.0 MPa | 2180 psi | at max load; ISO 527 |
A. Schulman FORMION™ FI 335 Ionomer Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 15.0 MPa | 2180 psi | at max load; ISO 527 |
A. Schulman FORMION™ FI 330 Ionomer Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 15.0 MPa | 2180 psi | at max load; ISO 527 |
A. Schulman FORMION™ FI 335 Ionomer Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 15.0 MPa | 2180 psi | at max load; ISO 527 |
A. Schulman FORMION™ FI 330 Ionomer Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 15.0 MPa | 2180 psi | at max load; ISO 527 |
A. Schulman FORMION™ FI 335 Ionomer Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 15.0 MPa | 2180 psi | at max load; ISO 527 |
A. Schulman FORMION™ FI 335 Ionomer Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 15.0 MPa | 2180 psi | at max load; ISO 527 |
A. Schulman FORMION™ FI 330 Ionomer Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 15.0 MPa | 2180 psi | at max load; ISO 527 |
A. Schulman FORMION™ FI 335 Ionomer Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 15.0 MPa | 2180 psi | ASTM D638/D412 |
Covestro Bayflex® MP-10000 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System 0.118 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
Tensile Strength, Ultimate | 15.0 MPa | 2180 psi | ASTM D412 |
Colorite Polymers CS6041GP Non Lead Wire and Cable Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Tensile Strength, Ultimate | 15.0 MPa | 2180 psi | |
BASF Lucalen® A 3110 M Ethylene/Acrylate Copolymer Economical composite films together with PE-LD; primers for aluminum/steel composites; coatings for paper board, aluminum and steel (e.g. for pipes used to transport petroleum, gas, etc.)Data was co.. |
|||
Tensile Strength, Ultimate | 15.0 - 35.0 MPa | 2180 - 5080 psi | |
ATG s.r.l. AU-EU Polyurethane Rubber |
|||
Tensile Strength, Ultimate | 15.0 MPa | 2180 psi | ASTM D638 |
ExxonMobil Escorene® LD-728 High EVA Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer with a low melting temperature and excellent strength properties and toughness.Applications: Injection molding; Foams.. |
|||
Tensile Strength, Ultimate | 15.0 MPa | 2180 psi | ASTM D638 |
ITW Plexus Plexus™ MA440 Methacrylate Adhesive Two-part, self-leveling adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies. |
|||
Tensile Strength, Ultimate | 15.0 MPa | 2180 psi | ASTM D638 |
Huntsman PE8010 Specialty Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Yields film with excellent draw down and machinability.Applications: Film extrusion: gel free film applications.FDA Notes: Conforms to FDA regulation 21 CFR 1.. |