Polymer Property : Dart Drop, Total Energy = 59.0 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop, Total Energy 80.0 J

@Temperature 23.0 °C
59.0 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® CFR9111 PC COPOLYMER
Lexan* CFR9111 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm and good flow capability. ..
Dart Drop, Total Energy 80.0 J

@Temperature 23.0 °C
59.0 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® CFR9111 PC COPOLYMER (Asia Pacific)
Lexan* CFR9111 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm and good flow capability. ..
Dart Drop, Total Energy 80.0 J

@Temperature 23.0 °C
59.0 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® CFR9111 PC COPOLYMER (Europe-Africa-Middle East)
Lexan* CFR9111 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm and good flow capability. ..
Dart Drop, Total Energy 80.0 J

@Temperature 23.0 °C
59.0 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer (Asia Pacific)
Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior ..
Dart Drop, Total Energy 80.0 J

@Temperature 23.0 °C
59.0 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® FST9705 PC Copolymer
High viscosity Proprietary Polycarbonate Ester, OSU 55/55 compliant, low smoke, flame retardant resin
Dart Drop, Total Energy 80.0 J

@Temperature 23.0 °C
59.0 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® FST9705 PC Copolymer (Asia Pacific)
High visocisty PC Copolymer, OSU 55/55 compliant, low smoke, flame retardant resin
Dart Drop, Total Energy 80.0 J

@Temperature 23.0 °C
59.0 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® FST9705 PC Copolymer (Europe-Africa-Middle East)
High viscosity PC Copolymer, OSU 55/55 compliant, low smoke, flame retardant resin
Dart Drop, Total Energy 80.0 J

@Temperature 23.0 °C
59.0 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® ML7686 PC (Asia Pacific)
Transparent Polycarbonate in limited colors. Excellent processability, super high flow. UL rated V-2 at 1.5mm.
Dart Drop, Total Energy 80.0 J

@Temperature 23.0 °C
59.0 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® ML7686 PC (Europe-Africa-Middle East)
Transparent Polycarbonate in limited colors. Excellent processability, super high flow. UL rated V-2 at 1.5mm.
Dart Drop, Total Energy 80.0 J

@Temperature 23.0 °C
59.0 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® ML7686E PC (Europe-Africa-Middle East)
Transparent Polycarbonate in natural color. Excellent processability, super high flow. UL compliant 94V-2 at 1.5mm.
Dart Drop, Total Energy 80.0 J

@Temperature 23.0 °C
59.0 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® SLX1431D PC Copolymer
Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.
Dart Drop, Total Energy 80.0 J

@Temperature 23.0 °C
59.0 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® SLX2231T PC Copolymer (Asia Pacific)
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors
Dart Drop, Total Energy 80.0 J

@Temperature 23.0 °C
59.0 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® SLX2431T PC Copolymer
Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors
Dart Drop, Total Energy 80.0 J

@Temperature 23.0 °C
59.0 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® SLX2431T PC Copolymer (Asia Pacific)
Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors
Dart Drop, Total Energy 80.0 J

@Temperature 23.0 °C
59.0 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® EXRL1061 PC (Asia Pacific)
Transparent Polycarbonate in natural color. Excellent processability, super high flow.
Dart Drop, Total Energy 80.0 J

@Temperature 23.0 °C
59.0 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer
Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior ..
Dart Drop, Total Energy 80.0 J

@Temperature 23.0 °C
59.0 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer (Europe-Africa-Middle East)
Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior ..
Dart Drop, Total Energy 80.0 J

@Temperature 23.0 °C
59.0 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® SLX1231T PC Copolymer (Asia Pacific)
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colors
Dart Drop, Total Energy 80.0 J

@Temperature 23.0 °C
59.0 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® SLX1431D PC Copolymer (Asia Pacific)
Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.
Dart Drop, Total Energy 80.0 J

@Temperature 23.0 °C
59.0 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® SLX2271T PC Copolymer
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors
Dart Drop, Total Energy 80.0 J

@Temperature 23.0 °C
59.0 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® SLX2271T PC Copolymer (Europe-Africa-Middle East)
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors
Dart Drop, Total Energy 80.0 J

@Thickness 3.20 mm
59.0 ft-lb

@Thickness 0.126 in
203m/min; ASTM D3763
LG Chemical Lupoy 1201-18 Polycarbonate Resin
Description: LUPOY PC 1201-18 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Dart Drop, Total Energy 80.0 J

@Temperature 23.0 °C
59.0 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC
Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing..
Dart Drop, Total Energy 80.0 J

@Temperature 23.0 °C
59.0 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC (Asia Pacific)
Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing..
Dart Drop, Total Energy 80.0 J

@Temperature 23.0 °C
59.0 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC (Europe-Africa-Middle East)
Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing..
Dart Drop, Total Energy 80.0 J
59.0 ft-lb
DIN 53443
Zell-Metall Engineering Plastics Zellamid 1400 (PET)
Zellamid® 1400 is the registered trademark of Zell-Metall’s partly crystalline thermoplastic Polyester based on Polyethylene Terephthalate.This PETP features outstanding dimensional stability, ..
Dart Drop, Total Energy 80.0 J
59.0 ft-lb
DIN 53443
Zell-Metall Engineering Plastics Zellamid 1400 (PET) at 50% RH
Zellamid® 1400 is the registered trademark of Zell-Metall’s partly crystalline thermoplastic Polyester based on Polyethylene Terephthalate.This PETP features outstanding dimensional stability, ..