Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 75.0 J @Temperature 23.0 °C |
55.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® FXD941A PC (Europe-Africa-Middle East) Transparent/translucent PC for light diffusion special effects. Color package may affect performance. |
|||
Dart Drop, Total Energy | 75.0 J @Temperature 23.0 °C |
55.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® FXE1414T PC Copolymer Clear PC-siloxane copolymer with excellent processability, for Visual fX capability in ""Energy"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color pac.. |
|||
Dart Drop, Total Energy | 75.0 J @Temperature 23.0 °C |
55.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® FXE1414T PC Copolymer (Asia Pacific) Clear PC-siloxane copolymer with excellent processability, for Visual fX capability in ""Energy"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color pac.. |
|||
Dart Drop, Total Energy | 75.0 J @Temperature 23.0 °C |
55.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® ML6412 PC Copolymer ML6412 is an impact modified PC resin with non-brominated, non-chlorinated flame retardant system. |
|||
Dart Drop, Total Energy | 75.0 J @Temperature 23.0 °C |
55.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® ML6412 PC Copolymer (Asia Pacific) ML6412 is an impact modified PC resin with non-brominated, non-chlorinated flame retardant system. |
|||
Dart Drop, Total Energy | 75.0 J @Temperature 23.0 °C |
55.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® 9925A PC (Asia Pacific) Lexan 9925A is a flame retardant transparent polycarbonate featuring non brominated and non chlorinated FR system with good flow and thin wall FR performance. It intended to meet WEEE/RoHS requireme.. |
|||
Dart Drop, Total Energy | 75.0 J @Temperature 23.0 °C |
55.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® EXL9414T PC Copolymer (Asia Pacific) Lexan* EXL9414T resin grade is a halogen-free flame retardant polycarbonate featuring transparency, -40 degree C ductility and UL-94 V0 rating for injection molding applications. Excellent impact co.. |
|||
Dart Drop, Total Energy | 75.0 J @Temperature 23.0 °C |
55.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® FXE9925A PC (Asia Pacific) Illuminate / edge glow color effect grade of Lexan 9925A. 9925A is a flame retardant transparent polycarbonate featuring non brominated and non chlorinated FR system with good flow and thin wall FR .. |
|||
Dart Drop, Total Energy | 75.0 J @Temperature 23.0 °C |
55.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® EXL9414T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL9414T resin grade is a halogen-free flame retardant polycarbonate featuring transparency, -40 degree C ductility and UL-94 V0 rating for injection molding applications. Excellent impact co.. |