Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 103 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 7.0 MFR, for thicker sections without sinks. UV stabilized for outdoor and lighting. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 104R PC (Asia Pacific) LEXAN 104R is a high viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information a.. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 121R PC (Asia Pacific) Nonhalogenated. 17.5 MFR, for small, intricate parts. Internal mold release. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 124 PC (Asia Pacific) 17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information and should not .. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 124R PC (Asia Pacific) LEXAN 124R is a low viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information an.. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 131 PC Nonhalogenated. 3.5 MFR. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 144 PC UL rated HB. 200 series recommended when V-2 rating required. 10.5 MFR. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will no longer be supported with bioco.. |
|||
Dart Drop, Total Energy | 169 J @Temperature 23.0 °C |
125 ft-lb @Temperature 73.4 °F |
ASTM D 3029 |
SABIC Innovative Plastics Lexan® 151R PC Lexan 151R resin is a high viscosicty, nonhalogenated resin designed to be a candidate for applications produced via extrusion or blow molding processing.This data was supplied by SABIC-IP for the A.. |
|||
Dart Drop, Total Energy | 169 J @Temperature 23.0 °C |
125 ft-lb @Temperature 73.4 °F |
ASTM D 3029 |
SABIC Innovative Plastics Lexan® 194 PC Nonhalogenated. 8.5 MFR. High impact. Thick wall sections. Opaques only. FDA food contact compliant in limited colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 201R PC 7.0 MFR, for thicker sections without sinks. Improved flame retardance. Internal mold release. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 223S PC (Asia Pacific) 17.5 MFR, for small, intricate parts. Improved flame retardance. Internal mold release. UV stabilized. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 241R PC (Asia Pacific) 10.5 MFR. Improved flame retardance. Internal mold release. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 920A PC Low viscosity injection moldable, flame retardant PC. Exceptional surface appearance. Clear, tints and opaque colors. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® HF1140R PC High flow grade. Heat stabilized. Enhanced level of mold release. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no longer be supported with biocompatib.. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® HP2C PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains m.. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® HP6NR PC (Europe-Africa-Middle East) Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no .. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® HP9NR PC Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. For blow molding .. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® LI1813R PC Low-viscosity multi-purpose PC having low levels of ionics species. Internal mold release and UV-stabilized. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | SABIC Method |
SABIC Innovative Plastics Lexan® LS2 PC (Asia Pacific) Automotive lens applications. Medium viscosity. UV-stabilized. Transparent colors only. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® OQ4320R PC Optical grade with UV cut-off up to 400 nm; greater optical purity than standard grades. For sunglass and sunvisor markets. Internal mold release. |
|||
Dart Drop, Total Energy | 169 J @Temperature 23.0 °C |
125 ft-lb @Temperature 73.4 °F |
ASTM D 3029 |
SABIC Innovative Plastics Lexan® OQ4620 PC Optical grade with UV cut-off up to 400 nm, greater optical purity than standard grades. For needs of sunglass and sunvisor markets.This data was supplied by SABIC-IP for the Americas region. |
|||
Dart Drop, Total Energy | 169 J @Temperature 23.0 °C |
125 ft-lb @Temperature 73.4 °F |
ASTM D 3029 |
SABIC Innovative Plastics Lexan® RL7517 PC FDA compliant (color limited). 2.5 MFR. Potable water/extrusion blowmolding applications.This data was supplied by SABIC-IP for the Americas region. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 144R PC (Asia Pacific) LEXAN 144R is a medium viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information.. |
|||
Dart Drop, Total Energy | 169 J @Temperature 23.0 °C |
125 ft-lb @Temperature 73.4 °F |
ASTM D 3029 |
SABIC Innovative Plastics Lexan® 151 PC (Asia Pacific) Nonhalogenated. 2.5 MFR. Blowmolding/extrusion.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Dart Drop, Total Energy | 169 J @Temperature 23.0 °C |
125 ft-lb @Temperature 73.4 °F |
ASTM D 3029 |
SABIC Innovative Plastics Lexan® 303 PC (Asia Pacific) Clear, high viscosity material designed to service severe environments of HID lighting.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 943 PC (Asia Pacific) Opaque colors, medium viscosity, superior flame retardance. UV-stabilized. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® 953 PC Opaque colors, high viscosity, superior flame retardance. UV-stabilized. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® HP1 PC High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® HP2NR PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no.. |
|||
Dart Drop, Total Energy | 169 J | 125 ft-lb | ASTM D3029 |
SABIC Innovative Plastics Lexan® HP4NR PC Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no m.. |