Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 80.0 J @Temperature 23.0 °C |
59.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® CFR9111 PC COPOLYMER Lexan* CFR9111 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm and good flow capability. .. |
|||
Dart Drop, Total Energy | 80.0 J @Temperature 23.0 °C |
59.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® CFR9111 PC COPOLYMER (Asia Pacific) Lexan* CFR9111 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm and good flow capability. .. |
|||
Dart Drop, Total Energy | 80.0 J @Temperature 23.0 °C |
59.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® CFR9111 PC COPOLYMER (Europe-Africa-Middle East) Lexan* CFR9111 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm and good flow capability. .. |
|||
Dart Drop, Total Energy | 80.0 J @Temperature 23.0 °C |
59.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer (Asia Pacific) Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior .. |
|||
Dart Drop, Total Energy | 80.0 J @Temperature 23.0 °C |
59.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® FST9705 PC Copolymer High viscosity Proprietary Polycarbonate Ester, OSU 55/55 compliant, low smoke, flame retardant resin |
|||
Dart Drop, Total Energy | 80.0 J @Temperature 23.0 °C |
59.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® FST9705 PC Copolymer (Asia Pacific) High visocisty PC Copolymer, OSU 55/55 compliant, low smoke, flame retardant resin |
|||
Dart Drop, Total Energy | 80.0 J @Temperature 23.0 °C |
59.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® FST9705 PC Copolymer (Europe-Africa-Middle East) High viscosity PC Copolymer, OSU 55/55 compliant, low smoke, flame retardant resin |
|||
Dart Drop, Total Energy | 80.0 J @Temperature 23.0 °C |
59.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® ML7686 PC (Asia Pacific) Transparent Polycarbonate in limited colors. Excellent processability, super high flow. UL rated V-2 at 1.5mm. |
|||
Dart Drop, Total Energy | 80.0 J @Temperature 23.0 °C |
59.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® ML7686 PC (Europe-Africa-Middle East) Transparent Polycarbonate in limited colors. Excellent processability, super high flow. UL rated V-2 at 1.5mm. |
|||
Dart Drop, Total Energy | 80.0 J @Temperature 23.0 °C |
59.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® ML7686E PC (Europe-Africa-Middle East) Transparent Polycarbonate in natural color. Excellent processability, super high flow. UL compliant 94V-2 at 1.5mm. |
|||
Dart Drop, Total Energy | 80.0 J @Temperature 23.0 °C |
59.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® SLX1431D PC Copolymer Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors. |
|||
Dart Drop, Total Energy | 80.0 J @Temperature 23.0 °C |
59.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® SLX2231T PC Copolymer (Asia Pacific) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Dart Drop, Total Energy | 80.0 J @Temperature 23.0 °C |
59.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® SLX2431T PC Copolymer Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Dart Drop, Total Energy | 80.0 J @Temperature 23.0 °C |
59.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® SLX2431T PC Copolymer (Asia Pacific) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Dart Drop, Total Energy | 80.0 J @Temperature 23.0 °C |
59.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® EXRL1061 PC (Asia Pacific) Transparent Polycarbonate in natural color. Excellent processability, super high flow. |
|||
Dart Drop, Total Energy | 80.0 J @Temperature 23.0 °C |
59.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior .. |
|||
Dart Drop, Total Energy | 80.0 J @Temperature 23.0 °C |
59.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer (Europe-Africa-Middle East) Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior .. |
|||
Dart Drop, Total Energy | 80.0 J @Temperature 23.0 °C |
59.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® SLX1231T PC Copolymer (Asia Pacific) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colors |
|||
Dart Drop, Total Energy | 80.0 J @Temperature 23.0 °C |
59.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® SLX1431D PC Copolymer (Asia Pacific) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors. |
|||
Dart Drop, Total Energy | 80.0 J @Temperature 23.0 °C |
59.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® SLX2271T PC Copolymer Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Dart Drop, Total Energy | 80.0 J @Temperature 23.0 °C |
59.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® SLX2271T PC Copolymer (Europe-Africa-Middle East) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Dart Drop, Total Energy | 80.0 J @Thickness 3.20 mm |
59.0 ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
LG Chemical Lupoy 1201-18 Polycarbonate Resin Description: LUPOY PC 1201-18 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Dart Drop, Total Energy | 80.0 J @Temperature 23.0 °C |
59.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Dart Drop, Total Energy | 80.0 J @Temperature 23.0 °C |
59.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC (Asia Pacific) Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Dart Drop, Total Energy | 80.0 J @Temperature 23.0 °C |
59.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC (Europe-Africa-Middle East) Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Dart Drop, Total Energy | 80.0 J | 59.0 ft-lb | DIN 53443 |
Zell-Metall Engineering Plastics Zellamid 1400 (PET) Zellamid® 1400 is the registered trademark of Zell-Metalls partly crystalline thermoplastic Polyester based on Polyethylene Terephthalate.This PETP features outstanding dimensional stability, .. |
|||
Dart Drop, Total Energy | 80.0 J | 59.0 ft-lb | DIN 53443 |