Mechanical Properties Metric English Comments
Tensile Strength 520 MPa

@Thickness 300 - 400 mm
75400 psi

@Thickness 11.8 - 15.7 in
long-transverse direction
Constellium Alumold® 500 Forged Aluminum
Forged thick blocks in Alumold® 500 have been developed to provide high and consistent strength across the thickness, good dimensional stability and excellent machinability, in order to respond to ..
Tensile Strength 520 MPa

@Thickness 240 - 305 mm
75400 psi

@Thickness 9.45 - 12.0 in
Tempers T651 / T652
Constellium Certal® SPC Aluminum
Certal® SPC has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important property in man..
Tensile Strength 520 MPa

@Thickness 325 - 400 mm
75400 psi

@Thickness 12.8 - 15.7 in
Temper T652
Constellium Certal® SPC Forged Aluminum
Certal® SPC forged has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important property..
Tensile Strength 520 MPa

@Thickness 400 - 450 mm
75400 psi

@Thickness 15.7 - 17.7 in
Temper T652
Constellium Certal® SPC Forged Aluminum
Certal® SPC forged has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important property..
Tensile Strength 520 MPa

@Thickness 120 - 140 mm
75400 psi

@Thickness 4.72 - 5.51 in
Typical Strength
Constellium Fortal® Aluminum Alloy
Fortal® plates are optimized to provide high mechanical strength, combined with good shape stability and excellent machinability. Typical applications include sheet forming tools, base plates for m..