Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength = 80.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 80.0 MPa

@Temperature 23.0 °C
11600 psi

@Temperature 73.4 °F
ISO 527
Premix Premi-Glas® 1286 Glass Reinforced SMC
Description: Premi-Glas® 1286 is a glass reinforced thermoset sheet molding compound designed for automotive under the hood applications. Key features and benefits: Designed for compression molding..
Tensile Strength 80.0 MPa

@Temperature 23.0 °C
11600 psi

@Temperature 73.4 °F
DAM; ASTM D638
DuPont Performance Polymers Zytel® 7301 NC010 Nylon 6  (Unverified Data**)
Zytel® 7301 NC010 is a general purpose, unlubricated polyamide 6 resin for extrusion applications.Information provided by DuPont Performance Polymers
Tensile Strength 80.0 MPa

@Temperature 175 °C
11600 psi

@Temperature 347 °F
DAM; ASTM D638
DuPont Performance Polymers Zytel® HTN 52G35HSL NC010 Polyphthalamide (PPA)
Zytel® HTN52G35HSL NC010 is a 35% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds.Information provided by DuPont Performance ..
Tensile Strength 80.0 MPa

@Temperature 23.0 °C
11600 psi

@Temperature 73.4 °F
ISO 527
BASF Ultradur® S 4090 G2 10% Glass Filled PBT
Description: Is a PBT + ASA, easy-flowing injection-molding grades with 10% glass fibers; for rigid, tough and dimensionally stable technical parts e. g. housings, consoles, contact carriers, covers..
Tensile Strength 80.0 MPa

@Strain 8.00 %,
Temperature 23.0 °C
11600 psi

@Strain 8.00 %,
Temperature 73.4 °F
50mm/min
BASF Ultramid® KR 4350 PA6/6T (Dry)
Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain con..
Tensile Strength 80.0 MPa

@Strain 9.00 %,
Temperature 100 °C
11600 psi

@Strain 9.00 %,
Temperature 212 °F
5mm/min
BASF Ultramid® KR 4355 G7 35% Glass Filled PA6/6T (Dry)
Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r..
Tensile Strength 80.0 MPa

@Strain 3.00 %,
Temperature 23.0 °C
11600 psi

@Strain 3.00 %,
Temperature 73.4 °F
ISO 527
BASF Ultramid® B3S HP PA6 (Dry)
Ultramid B3S HP is a easy flowing, finely crystalline, injection molding PA6 for fast processing
Copyright © lookpolymers.com All Rights Reserved