Polymer Property : Tensile Strength = 480 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 480 MPa

@Thickness 101.6 - 127 mm
69600 psi

@Thickness 4.000 - 5.00 in
Typical Strength
Constellium Alumold® 350 Aluminum
Alumold-350® has been specifically developed to achieve the best combination of strength at low and high temperatures, together with a good shape stability and machinability. Alumold-350® is parti..
Tensile Strength 480 MPa

@Thickness 450 - 700 mm
69600 psi

@Thickness 17.7 - 27.6 in
long-transverse direction
Constellium Alumold® 500 Forged Aluminum
Forged thick blocks in Alumold® 500 have been developed to provide high and consistent strength across the thickness, good dimensional stability and excellent machinability, in order to respond to ..
Tensile Strength 480 MPa

@Thickness 450 - 700 mm
69600 psi

@Thickness 17.7 - 27.6 in
Temper T652
Constellium Certal® SPC Forged Aluminum
Certal® SPC forged has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important property..
Tensile Strength >= 480 MPa

@Thickness 120 - 140 mm
>= 69600 psi

@Thickness 4.72 - 5.51 in
Constellium Fortal® Aluminum Alloy
Fortal® plates are optimized to provide high mechanical strength, combined with good shape stability and excellent machinability. Typical applications include sheet forming tools, base plates for m..
Tensile Strength >= 480 MPa

@Thickness 160 - 180 mm
>= 69600 psi

@Thickness 6.30 - 7.09 in
Constellium Fortal® Aluminum Alloy
Fortal® plates are optimized to provide high mechanical strength, combined with good shape stability and excellent machinability. Typical applications include sheet forming tools, base plates for m..