Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 65.0 - 75.0 MPa @Temperature 100 °C |
9430 - 10900 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURASBOND 85 Moldable Refractory Material Description: Curasbond 85 is a pouring repairmass, characterized by excellent resistance to aluminum and rapid hardening. The product is supplied in two components: a dry powder and a liquid. It can.. |
|||
Compressive Strength | 65.0 - 75.0 MPa @Temperature 1000 °C |
9430 - 10900 psi @Temperature 1830 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 150 AC Dense Refractory Castable Description: Curon 150 AC is a coarse castable for use up to 1500°C with a high strength.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast. |
|||
Compressive Strength | 65.0 - 75.0 MPa @Temperature 100 °C |
9430 - 10900 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 150 HS Dense Refractory Castable Description: Dense refractory castableRemarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information provided by Gouda Vuurvast. |
|||
Compressive Strength | 65.0 - 75.0 MPa @Temperature 100 °C |
9430 - 10900 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 150 RN Dense Refractory Castable Description: This on sintered bauxite and low-iron alumina cement based castable contains stainless steel fibers, what results in a very good mechanical strength.Remarks: These values apply to cast .. |
|||
Compressive Strength | 65.0 - 75.0 MPa @Temperature 100 °C |
9430 - 10900 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 160 HF Dense Refractory Castable Description: This castable has a high volume stability and keeps its strength up to high temperatures. In addition, Curon 160 HF has an excellent thermal shock resistance. It is largely used in the .. |
|||
Compressive Strength | 65.0 - 75.0 MPa @Temperature 100 °C |
9430 - 10900 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast FLUCON 150 Dense Self Flowing Refractory Castable Description: Flucon 150 is a self-flowing low cement castable based on sintered bauxite.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast. |
|||
Compressive Strength | 65.0 - 75.0 MPa @Temperature 100 °C |
9430 - 10900 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast FLUCON 160 K Dense Self Flowing Refractory Castable Description: Flucon 160 K is a self-flowing low cement castable based on silicon carbide. This castable is characterized by high strength high abrasion resistance and excellent thermal shock resista.. |
|||
Compressive Strength | 65.0 - 75.0 MPa @Temperature 100 °C |
9430 - 10900 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 130 Dense Vibrating Refractory Castable Description: Vibron 130 is a vibrating castable with a low cement content, based on abrasion resistant spinel grains.Remarks: Indicated values apply to vibrated products.Information provided by Goud.. |
|||
Compressive Strength | 65.0 - 75.0 MPa @Temperature 100 °C |
9430 - 10900 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 13 S Dense Refractory Castable Description: Curon 13 S is a spinel based castable with a very low silica content and therefore it is suitable for direct contact with all kinds of aluminum/alloys and fluxes in aluminum melting/hol.. |
|||
Compressive Strength | 65.0 - 75.0 MPa @Temperature 100 °C |
9430 - 10900 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 160 HS Dense Refractory Castable Description: Because of the selection of raw materials, this castable has a high volume stability and a high strength up to high temperatures. In addition, Curon 160 HS has an excellent thermal shoc.. |
|||
Compressive Strength | 65.0 - 75.0 MPa @Temperature 100 °C |
9430 - 10900 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 160 HSC Dense Refractory Castable Description: Curon 160 HSC is a coarse abrasion resistant castable to be used up to 1600°C in reducing conditions.Remarks: These values apply to cast products.Information provided by Gouda Vuurva.. |
|||
Compressive Strength | 65.0 - 75.0 MPa @Temperature 100 °C |
9430 - 10900 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 160 K 50 Dense Vibrating Refractory Castable Description: Vibron 160 K 50 is a low cement castable based on silicon carbide and characterized by a very good thermal conductivity, high abrasion resistance and a good oxidation resistance up to 1.. |
|||
Compressive Strength | 65.0 - 75.0 MPa @Temperature 100 °C |
9430 - 10900 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 160 K Dense Vibrating Refractory Castable Description: Vibron 160 K is a low cement castable based on silicon carbide and characterized by a very good thermal conductivity and high abrasion resistance. The thermal shock resistance is excell.. |
|||
Compressive Strength | 65.0 - 75.0 MPa @Temperature 100 °C |
9430 - 10900 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 162 K Sp Dense Vibrating Refractory Silicon Carbide Castable Vibron 162 K Sp is a low cement castable based on silicon carbide. This castable is characterized by a very good thermal conductivity, a high abrasion resistance and high resistance against oxidatio.. |
|||
Compressive Strength | 65.0 - 75.0 MPa @Temperature 100 °C |
9430 - 10900 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 180 RAPID Dense Vibrating Refractory Castable Description: Vibron 180 Rapid is a low cement castable based on corundum with a special addition to enable a faster heating schedule. The material is supplied in two components. The B component cont.. |
|||
Compressive Strength | 65.0 - 75.0 MPa @Temperature 100 °C |
9430 - 10900 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast FLUCON 160 H Dense Self Flowing Refractory Castable Description: Flucon 160 H is a self-flowing low cement castable on high fired high alumina grog base, characterized by a high strength and good thermal shock resistance.Remarks: These values apply t.. |