Mechanical Properties Metric English Comments
Compressive Strength 300 MPa

@Temperature 23.0 °C
43500 psi

@Temperature 73.4 °F
ISO 604
Victrex® PEEK 150CA30 30% Carbon Fiber Reinforced
Product Description: High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, FDA food contact c..
Compressive Strength 300 MPa

@Temperature 23.0 °C
43500 psi

@Temperature 73.4 °F
ISO 604
Victrex® PEEK 450CA30 30% Carbon Fiber Reinforced
General purpose, 30% carbon fiber reinforced, pelletized grade for injection molding.Information provided by Victrex.
Compressive Strength 300 MPa

@Temperature 23.0 °C
43500 psi

@Temperature 73.4 °F
ISO 604
Victrex® PEEK 90CA30 Polyetheretherketone, 30% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 30% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food cont..
Compressive Strength 300 MPa

@Temperature 23.0 °C
43500 psi

@Temperature 73.4 °F
ISO 604
Victrex® PEEK -HT™ 22CA30 PolyEtherKetone, 30% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact com..
Compressive Strength 300 MPa

@Thickness 7.00 mm
43500 psi

@Thickness 0.276 in
LT Direction
Aleris AA5024-H116 Aluminum Magnesium Scandium Alloy
Features good weldability, excellent damage tolerance, good corrosion resistance, creep-formability. Aleris AlMgSc alloy AA5024 H116 allows simplification of the manufacturing process of aircraft f..
Compressive Strength 300 MPa

@Temperature 23.0 °C
43500 psi

@Temperature 73.4 °F
Dry; EN2850B
Hexcel® HexTOOL™ M61 Quasi-isotropic High Temperature Prepreg Tooling Compound
HexTOOL™ Tooling Compound is randomly layered strips of uni-directional prepreg which is consolidated into rolled goods. It can be utilized as multi-ply quasi-isotropic hand lay-up, and subsequentl..