Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 100 MPa @Strain 5 % |
14500 psi @Strain 5 % |
ISO 604 |
Quadrant EPP Ertalon® 66 SA PA 66, extruded (ISO Data) Material with a higher mechanical strength, stiffness, heat and wear resistance than Ertalon 6 SA. It also has a better creep resistance but its impact strength and mechanical damping ability is red.. |
|||
Compressive Strength | 100 MPa @Strain 5 % |
14500 psi @Strain 5 % |
ISO 604 |
Quadrant EPP Nylatron® GS PA 6 + MoS2, extruded (ISO Data) The addition of MoS2 renders this material somewhat stiffer, harder and dimensionally more stable than Ertalon 66 SA, but results in some loss of impact strength. The nucleating effect of the molybd.. |
|||
Compressive Strength | 100 - 120 MPa @Temperature 1300 °C |
14500 - 17400 psi @Temperature 2370 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 130 Dense Vibrating Refractory Castable Description: Vibron 130 is a vibrating castable with a low cement content, based on abrasion resistant spinel grains.Remarks: Indicated values apply to vibrated products.Information provided by Goud.. |
|||
Compressive Strength | 100 - 120 MPa @Temperature 1300 °C |
14500 - 17400 psi @Temperature 2370 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 140 Dense Vibrating Refractory Castable Description: Vibron 140 is a low cement castable, based on high quality chamotte.Remarks: Indicated values apply to vibrated products.Information provided by Gouda Vuurvast. |
|||
Compressive Strength | 100 - 120 MPa @Temperature 1400 °C |
14500 - 17400 psi @Temperature 2550 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 160 Dense Vibrating Refractory Castable Description: Vibron 160 is a low cement vibrating castable on andalusite base, characterized by a high strength and excellent thermal shock resistance.Remarks: Indicated values apply to vibrated pro.. |
|||
Compressive Strength | 100 - 120 MPa @Temperature 1400 °C |
14500 - 17400 psi @Temperature 2550 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 160 H Dense Vibrating Refractory Castable Description: Vibron 160 H is a low cement castable based on high fired high alumina grog and characterized by a high strength and good thermal shock resistance.Remarks: Indicated values apply to vib.. |
|||
Compressive Strength | 100 - 120 MPa @Temperature 1400 °C |
14500 - 17400 psi @Temperature 2550 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 165 Dense Vibrating Refractory Castable Description: Vibron 165 is a low cement castable based on andalusite and especially fit for the production of prefab elements.Remarks: Indicated values apply to vibrated products.Information provide.. |
|||
Compressive Strength | 100 - 120 MPa @Temperature 1400 °C |
14500 - 17400 psi @Temperature 2550 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 170 M Dense Vibrating Refractory Castable Description: Vibron 170 is a low cement castable based on synthetic mullite grog and is characterized by a high strength, excellent thermal shock resistance and high resistance to liquid slags.Remar.. |
|||
Compressive Strength | 100 - 120 MPa @Temperature 1400 °C |
14500 - 17400 psi @Temperature 2550 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 160 H RAPID Dense Vibrating Refractory Castable Description: Vibron 160 H Rap is a low cement castable based on high fired high alumina grog and characterized by a high strength and good thermal shock resistance. Because of special additives, thi.. |
|||
Compressive Strength | 100 - 120 MPa @Temperature 1400 °C |
14500 - 17400 psi @Temperature 2550 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 160 K 50 Dense Vibrating Refractory Castable Description: Vibron 160 K 50 is a low cement castable based on silicon carbide and characterized by a very good thermal conductivity, high abrasion resistance and a good oxidation resistance up to 1.. |
|||
Compressive Strength | 100 - 120 MPa @Temperature 1400 °C |
14500 - 17400 psi @Temperature 2550 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 160 K Dense Vibrating Refractory Castable Description: Vibron 160 K is a low cement castable based on silicon carbide and characterized by a very good thermal conductivity and high abrasion resistance. The thermal shock resistance is excell.. |
|||
Compressive Strength | 100 - 120 MPa @Temperature 1400 °C |
14500 - 17400 psi @Temperature 2550 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 162 K Sp Dense Vibrating Refractory Silicon Carbide Castable Vibron 162 K Sp is a low cement castable based on silicon carbide. This castable is characterized by a very good thermal conductivity, a high abrasion resistance and high resistance against oxidatio.. |
|||
Compressive Strength | 100 - 120 MPa @Temperature 1400 °C |
14500 - 17400 psi @Temperature 2550 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 170 M RAPID Dense Vibrating Refractory Castable Description: Vibron 170 M Rapid is a low cement castable based on synthetic mullite grog and is characterized by a high strength, excellent thermal shock resistance and high resistance to liquid sla.. |
|||
Compressive Strength | 100 MPa @Temperature 110 °C |
14500 psi @Temperature 230 °F |
Cold Crushing |
Sharadaa Ceramics VELECRETE RC 105 Rodding Castables Description: The Rodding Castables offered by us are user friendly in nature and does not require high energy mixing machines and vibrators. Free flowing in nature, these castables are designed in c.. |
|||
Compressive Strength | 100 MPa @Temperature 1400 °C |
14500 psi @Temperature 2550 °F |
Cold Crushing |
Sharadaa Ceramics VELECRETE RC 105 Rodding Castables Description: The Rodding Castables offered by us are user friendly in nature and does not require high energy mixing machines and vibrators. Free flowing in nature, these castables are designed in c.. |
|||
Compressive Strength | 100 MPa @Temperature 1000 °C |
14500 psi @Temperature 1830 °F |
Cold Crushing |
Sharadaa Ceramics VELECRETE RC 108 Rodding Castables Description: The Rodding Castables offered by us are user friendly in nature and does not require high energy mixing machines and vibrators. Free flowing in nature, these castables are designed in c.. |
|||
Compressive Strength | 100 MPa @Temperature 200 °C |
14500 psi @Temperature 392 °F |
|
Elisto THERMOSTAR® LC 6000 Insulation Material Pattern material. Insulation materials for mechanical engineering.Information provided by elisto |