Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 87.0 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.600 GPa

@Temperature 120 °C
87.0 ksi

@Temperature 248 °F
LATI Latamid 6 H-V0 PA 6, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good surface appearance.Availability: Africa & Middle East; Asi..
Tensile Modulus 0.600 GPa

@Temperature 150 °C
87.0 ksi

@Temperature 302 °F
LATI Latamid 66 B H-V0 PA 66, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. High fluidity. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Blended with PA6.Availability: Africa & Middle East..
Tensile Modulus 0.600 GPa

@Temperature 60.0 °C
87.0 ksi

@Temperature 140 °F
LATI Latene® 7-V2 PP Homopolymer, Flame Retardant
Polypropylene homopolymer (PPh) based compound. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A..
Tensile Modulus 0.600 GPa

@Temperature 120 °C
87.0 ksi

@Temperature 248 °F
LATI Kelon® B FR H CET/05-V2HF PA 6, Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free.Availability: Africa & Middle East; Asia Pacific; Eur..
Tensile Modulus 0.600 GPa

@Temperature 60.0 °C
87.0 ksi

@Temperature 140 °F
LATI Latene® EP 7-V2 PP Copolymer, Flame Retardant
Polypropylene copolymer (PPc) based compound. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ame..
Tensile Modulus 0.600 GPa

@Temperature 120 °C
87.0 ksi

@Temperature 248 °F
LATI Later 4-V0HF1 PBT, Flame Retardant
Polybutylene Terephthalate (PBT) based compound. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ..
Tensile Modulus 0.600 GPa

@Temperature 23.0 °C
87.0 ksi

@Temperature 73.4 °F
ASTM D 638
Saint-Gobain Meldin® 2030 Bearing
General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Series ca..
Tensile Modulus 0.600 GPa

@Temperature 260 °C
87.0 ksi

@Temperature 500 °F
ASTM D 638
Saint-Gobain Meldin® 2030 Bearing
General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Series ca..
Tensile Modulus 0.600 GPa

@Temperature 60.0 °C
87.0 ksi

@Temperature 140 °F
LATI Later 4E61 PBT
Polybutylene Terephthalate (PBT). Toughened. Good impact resistance even at low temperature.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided..