Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.70 GPa @Temperature 23.0 °C |
827 ksi @Temperature 73.4 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® 73G30HSL BK261 Nylon 6
(Unverified Data**) Zytel® 73G30HSL BK261 is a 30% glass fiber reinforced, heat stabilized, lubricated, black polyamide 6 for injection molding. It has excellent surface appearance and gloss.Information provided by Du.. |
|||
Tensile Modulus | 5.70 GPa @Temperature 23.0 °C |
827 ksi @Temperature 73.4 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® 73G30T NC010 Nylon 6
(Unverified Data**) Zytel® 73G30T NC010 is a 30% glass fiber reinforced, toughened polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 5.70 GPa @Temperature 90.0 °C |
827 ksi @Temperature 194 °F |
|
LATI Laramid G/15 PPA, 15% Glass Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; .. |
|||
Tensile Modulus | 5.70 GPa @Temperature 90.0 °C |
827 ksi @Temperature 194 °F |
|
LATI Larpeek 10 G/15 PEEK, 15% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Tensile Modulus | 5.70 GPa @Temperature 60.0 °C |
827 ksi @Temperature 140 °F |
|
LATI Latamid 66 E21 G/30 PA 66, 30% Glass Fiber Reinforced Polyamide 66 (PA66) based compound. Toughened. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici.. |
|||
Tensile Modulus | 5.70 GPa @Temperature 60.0 °C |
827 ksi @Temperature 140 °F |
|
LATI Latene® AG3H2W G/30-V0E PP Homopolymer, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polypropylene homopolymer (PPh) based compound. Chemical grafting Heat stabilized. Metal stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE freeAvailability: A.. |
|||
Tensile Modulus | 5.70 GPa @Temperature 60.0 °C |
827 ksi @Temperature 140 °F |
|
LATI Later 4 G/20 PBT, 20% Glass Fiber Reinforced Polybutylene Terephthalate (PBT) based compound. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast.. |
|||
Tensile Modulus | 5.70 GPa @Temperature 90.0 °C |
827 ksi @Temperature 194 °F |
|
LATI Latilon 28D G/20-V0 PC, 20% Glass Fiber Reinforced, Flame Retardant Polycarbonate (PC) based compound. Glass fibers. UL94 V-0 classified, brominated and chlorinated halogens-based flame retardants free. Low smoke density and low toxicity index. High dimensional stab.. |
|||
Tensile Modulus | 5.70 GPa @Temperature 23.0 °C |
827 ksi @Temperature 73.4 °F |
5mm/min (0.2in/min); ASTM D638 |
DuPont Performance Polymers Delrin® 577 BK000 Acetal Homopolymer
(Unverified Data**) Delrin® 577 BK000 is a medium viscosity acetal homopolymer containing 20% glass fiber filler, with high stiffness, low warpage and low creep for superior performance at elevated temperature. It con.. |