Mechanical Properties Metric English Comments
Tensile Modulus 6.90 GPa

@Temperature 23.0 °C
1000 ksi

@Temperature 73.4 °F
LATI Laril 13 G/20-V1 PPOm, 20% Glass Fiber Reinforced, Flame Retardant
Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. High dimensional stability. Good thermal..
Tensile Modulus 6.90 GPa

@Temperature 60.0 °C
1000 ksi

@Temperature 140 °F
LATI Laril 13 G/30 PPOm, 30% Glass Fiber Reinforced
Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. Low thermal expansion coefficient. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; ..
Tensile Modulus 6.90 GPa

@Temperature 120 °C
1000 ksi

@Temperature 248 °F
LATI Latamid 6 H2 G/50 PA 6, 50% Glass Fiber Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopla..
Tensile Modulus 6.90 GPa

@Temperature 90.0 °C
1000 ksi

@Temperature 194 °F
LATI Latamid SP2 H2 G/45 PA 6.12, 45% Glass Fiber Reinforced, Heat Stabilized
Polyamide 6.12 (PA6.12) based compound. Heat stabilized. Glass fibers. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provi..
Tensile Modulus 6.90 GPa

@Temperature 60.0 °C
1000 ksi

@Temperature 140 °F
LATI Later 4 G/30 PBT, 30% Glass Fiber Reinforced
Polybutylene Terephthalate (PBT) based compound. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast..
Tensile Modulus 6.90 GPa

@Temperature 23.0 °C
1000 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® 80G25HS BK117 Nylon 66  (Unverified Data**)
Zytel® 80G25HS BK117 is a 25% glass fiber reinforced, toughened, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Modulus 6.90 GPa

@Temperature 60.0 °C
1000 ksi

@Temperature 140 °F
LATI Latamid 66 H2 G/25-V0KB3 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn..
Copyright © lookpolymers.com All Rights Reserved