Mechanical Properties Metric English Comments
Tensile Modulus 4.60 GPa

@Temperature 23.0 °C
667 ksi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Minlon® 73GM40 NC010 Nylon 6  (Unverified Data**)
Minlon® 73GM40 NC010 is a 40% mineral/glass reinforced, heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Modulus 4.60 GPa

@Temperature 90.0 °C
667 ksi

@Temperature 194 °F
LATI Latamid 6 H2 G/30-V0HF1 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good electrical properties.Availability: Africa &..
Tensile Modulus 4.60 GPa

@Temperature 120 °C
667 ksi

@Temperature 248 °F
LATI Latamid 6 H2 G/35 PA 6, 35% Glass Fiber Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibersAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast..
Tensile Modulus 4.60 GPa

@Temperature 23.0 °C
667 ksi

@Temperature 73.4 °F
LATI Latamid 66 H2E21 G/13 PA 66, 13% Glass Fiber Reinforced
Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. Glass fibers. High impact resistance. Good impact resistance even at low temperature.Availability: Africa & Middle East; Asia Pacific;..
Tensile Modulus 4.60 GPa

@Temperature 23.0 °C
667 ksi

@Temperature 73.4 °F
LATI Lapex A G/10 PES, 10% Glass Fiber Reinforced
Polyether Sulfone (PES) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ..
Tensile Modulus 4.60 GPa

@Temperature 150 °C
667 ksi

@Temperature 302 °F
LATI Lapex R G/20 PPSU, 20% Glass Reinforced
Polyphenylene Sulfone (PPSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin A..
Tensile Modulus 4.60 GPa

@Temperature 90.0 °C
667 ksi

@Temperature 194 °F
LATI Latamid 6 CUVHPX10 G/35 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. High viscosity. Toughened. Glass fibers. Heat stabilized. UV stabilized. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No..
Copyright © lookpolymers.com All Rights Reserved