Polymer Property : Tensile Modulus = 2.30 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 2.30 GPa

@Temperature 23.0 °C
334 ksi

@Temperature 73.4 °F
ASTM-D638
Ineos ABS Lustran® LK197 ABS, Extrusion Grade
Lustran® ABS LK197 resin is a high-gloss, medium-impact extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It provides a superior balance between rigidity and impact strength, as well as e..
Tensile Modulus 2.30 GPa

@Temperature 60.0 °C
334 ksi

@Temperature 140 °F
LATI Lasulf PSU
Polysulfone (PSU). Unfilled. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformati..
Tensile Modulus 2.30 GPa

@Temperature 150 °C
334 ksi

@Temperature 302 °F
LATI Kelon® B FR H CET/30-V0 PA 6, Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Low thermal expansion coefficient. Very high dimensional stab..
Tensile Modulus 2.30 GPa

@Temperature 23.0 °C
334 ksi

@Temperature 73.4 °F
LATI Lastilac AR-V0E ABS, Flame Retardant
Acrylonitrile-Butadiene-Styrene copolymer (ABS) based compound. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very high dimensional stability. Very good surface appearance.Av..
Tensile Modulus 2.30 GPa

@Temperature 60.0 °C
334 ksi

@Temperature 140 °F
LATI Latan 13 S/30 POM, 30% Glass Bead Reinforced
Polyoxymethylene (POM) based compound. Glass beads. Medium viscosity. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro..
Tensile Modulus 2.30 GPa

@Temperature 23.0 °C
334 ksi

@Temperature 73.4 °F
LATI Later 4-V0HF1 PBT, Flame Retardant
Polybutylene Terephthalate (PBT) based compound. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ..
Tensile Modulus 2.30 GPa

@Temperature 120 °C
334 ksi

@Temperature 248 °F
ISO 527
DuPont Performance Polymers Crastin® HR5315HF NC010 PBT  (Unverified Data**)
Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis..
Tensile Modulus 2.30 GPa

@Temperature 120 °C
334 ksi

@Temperature 248 °F
LATI Latamid 66 H2 G/25-V0KB4 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn..