Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 18.0 GPa @Temperature 23.0 °C |
2610 ksi @Temperature 73.4 °F |
|
LATI Larpeek 10 G/50 PEEK, 50% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Tensile Modulus | 18.0 GPa @Temperature 60.0 °C |
2610 ksi @Temperature 140 °F |
|
LATI Larton GCE/600 PPS, Glass/Mineral Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers / Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa .. |
|||
Tensile Modulus | 18.0 GPa @Temperature 23.0 °C |
2610 ksi @Temperature 73.4 °F |
|
LATI Larpeek 10 K/20 PEEK, 20% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Tensile Modulus | 18.0 GPa @Temperature 23.0 °C |
2610 ksi @Temperature 73.4 °F |
|
LATI Larton L K/20 L-PPS, 20% Carbon Fiber Reinforced Linear Polyphenylene Sulfide (L-PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle.. |
|||
Tensile Modulus | 18.0 GPa @Temperature 23.0 °C |
2610 ksi @Temperature 73.4 °F |
|
LATI Latigloss 57 G/50 F2 PPA, 50% Glass Fiber Reinforced Product with high mechanical properties and exceptional surface finish based on Semi-aromatic polyamide (PPA). Glass fibers. Potentially suitable for food/medical contact application. Availability: .. |
|||
Tensile Modulus | 18.0 GPa @Temperature 60.0 °C |
2610 ksi @Temperature 140 °F |
|
LATI Latigloss 66 H2 G/60 PA 66, 60% Glass Fiber Reinforced, Heat Stabilized Product with high mechanical properties and exceptional surface finish based on Polyamide 66 (PA66). Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am.. |
|||
Tensile Modulus | 18.0 GPa @Temperature 23.0 °C |
2610 ksi @Temperature 73.4 °F |
|
LATI Latilon 28D K/40 PC, 40% Carbon Fiber Reinforced Polycarbonate (PC) based compound. Carbon fiber. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided b.. |
|||
Tensile Modulus | 18.0 GPa @Temperature 177 °C |
2610 ksi @Temperature 351 °F |
|
Hexcel® F161 Epoxy Resin, 120 Glass Fabric Hexcel designation: 120-38"-F161; Fiber: 450-1/2Information provided by HexCel |
|||
Tensile Modulus | 18.0 GPa @Temperature 150 °C |
2610 ksi @Temperature 302 °F |
ISO 527-1 |
Vyncolit Neopreg Kinel® SK4525 S5 Glass Fiber Reinforced Molding Compound BMI molding compound long glass fiber reinforced with excellent mechanical and thermal properties. Especially suited to be used for injection molding.Information provided by Sumitomo Bak North Ameri.. |