Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.90 GPa @Temperature 23.0 °C |
276 ksi @Temperature 73.4 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Minlon® 12TA BKB124 Nylon 66
(Unverified Data**) Minlon® 12TA BKB124 is a 32% mineral reinforced, toughened, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 1.90 GPa @Temperature 90.0 °C |
276 ksi @Temperature 194 °F |
|
LATI Kelon® B H CER/30 PA 6, 30% Mineral Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. Very high dimensional stability. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ame.. |
|||
Tensile Modulus | 1.90 GPa @Temperature 90.0 °C |
276 ksi @Temperature 194 °F |
|
LATI Lastilac 10 ABS/PC ABS/PC Blend (ABS/PC). Unfilled. Very good surface appearance. High impact resistance. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaI.. |
|||
Tensile Modulus | 1.90 GPa @Temperature 150 °C |
276 ksi @Temperature 302 °F |
|
LATI Lasulf PSU Polysulfone (PSU). Unfilled. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformati.. |
|||
Tensile Modulus | 1.90 GPa @Temperature 120 °C |
276 ksi @Temperature 248 °F |
|
LATI Latamid 66 E21 G/15 PA 66, 15% Glass Fiber Reinforced Polyamide 66 (PA66) based compound. Toughened. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici.. |
|||
Tensile Modulus | 1.90 GPa @Temperature 60.0 °C |
276 ksi @Temperature 140 °F |
|
LATI Latamid 66 PA 66 Polyamide 66 (PA66). Unfilled.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A. |
|||
Tensile Modulus | 1.90 GPa @Temperature 60.0 °C |
276 ksi @Temperature 140 °F |
|
LATI Lastilac AR-V0E ABS, Flame Retardant Acrylonitrile-Butadiene-Styrene copolymer (ABS) based compound. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very high dimensional stability. Very good surface appearance.Av.. |
|||
Tensile Modulus | 1.90 GPa @Temperature 23.0 °C |
276 ksi @Temperature 73.4 °F |
|
LATI Latan 3E71 POM Polyoxymethylene (POM). Toughened. High viscosity. Good elongation and impact resistanceAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by .. |
|||
Tensile Modulus | 1.90 GPa @Temperature 23.0 °C |
276 ksi @Temperature 73.4 °F |
|
LATI Latene® 7H2-V2HF PP Homopolymer, Heat Stabilized, Flame Retardant Polypropylene homopolymer (PPh) based compound. Heat stabilized. UL94 V-2 classified, halogens-based flame retardants free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No.. |
|||
Tensile Modulus | 1.90 GPa @Temperature 23.0 °C |
276 ksi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® ST801AW BK195 Nylon 66
(Unverified Data**) Zytel® ST801AW BK195 is a Super Tough, weatherable, easy flow and processing friendly, black polyamide 66 resin for injection molding. It offers the best resistance to outdoor exposure.Information.. |
|||
Tensile Modulus | 1.90 GPa @Temperature 23.0 °C |
276 ksi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® ST801AW NC010 Nylon 66
(Unverified Data**) Zytel® ST801AW NC010 is a Super Tough, high performance polyamide 66 resin. It is UV stabilized and when appropriately colored offers the best resistance to indirect sunlight in automotive interior.. |
|||
Tensile Modulus | 1.90 GPa @Temperature 23.0 °C |
276 ksi @Temperature 73.4 °F |
|
LATI Later 4E61 PBT Polybutylene Terephthalate (PBT). Toughened. Good impact resistance even at low temperature.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |
|||
Tensile Modulus | 1.90 GPa @Temperature 23.0 °C |
276 ksi @Temperature 73.4 °F |
|
LATI Latiblend 7587 E61-V0 PBT/PC, Flame Retardant Blend based on Polybutylene Terephthalate (PBT) / Polycarbonate (PC). Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very high dimensional stability. High impact re.. |
|||
Tensile Modulus | 1.90 GPa @Temperature 90.0 °C |
276 ksi @Temperature 194 °F |
|
LATI Latilon 30D-V0 PC, Flame Retardant Polycarbonate (PC) based compound. UL94 V-0 classified, brominated and chlorinated halogens-based flame retardants free. Low smoke density and low toxicity index. Very high dimensional stability. Ve.. |