Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.600 GPa @Temperature 120 °C |
87.0 ksi @Temperature 248 °F |
|
LATI Latamid 6 H-V0 PA 6, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good surface appearance.Availability: Africa & Middle East; Asi.. |
|||
Tensile Modulus | 0.600 GPa @Temperature 150 °C |
87.0 ksi @Temperature 302 °F |
|
LATI Latamid 66 B H-V0 PA 66, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. High fluidity. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Blended with PA6.Availability: Africa & Middle East.. |
|||
Tensile Modulus | 0.600 GPa @Temperature 60.0 °C |
87.0 ksi @Temperature 140 °F |
|
LATI Latene® 7-V2 PP Homopolymer, Flame Retardant Polypropylene homopolymer (PPh) based compound. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A.. |
|||
Tensile Modulus | 0.600 GPa @Temperature 120 °C |
87.0 ksi @Temperature 248 °F |
|
LATI Kelon® B FR H CET/05-V2HF PA 6, Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free.Availability: Africa & Middle East; Asia Pacific; Eur.. |
|||
Tensile Modulus | 0.600 GPa @Temperature 60.0 °C |
87.0 ksi @Temperature 140 °F |
|
LATI Latene® EP 7-V2 PP Copolymer, Flame Retardant Polypropylene copolymer (PPc) based compound. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ame.. |
|||
Tensile Modulus | 0.600 GPa @Temperature 120 °C |
87.0 ksi @Temperature 248 °F |
|
LATI Later 4-V0HF1 PBT, Flame Retardant Polybutylene Terephthalate (PBT) based compound. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ.. |
|||
Tensile Modulus | 0.600 GPa @Temperature 23.0 °C |
87.0 ksi @Temperature 73.4 °F |
ASTM D 638 |
Saint-Gobain Meldin® 2030 Bearing General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Series ca.. |
|||
Tensile Modulus | 0.600 GPa @Temperature 260 °C |
87.0 ksi @Temperature 500 °F |
ASTM D 638 |
Saint-Gobain Meldin® 2030 Bearing General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Series ca.. |
|||
Tensile Modulus | 0.600 GPa @Temperature 60.0 °C |
87.0 ksi @Temperature 140 °F |
|
LATI Later 4E61 PBT Polybutylene Terephthalate (PBT). Toughened. Good impact resistance even at low temperature.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |