Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 92.0 MPa @Temperature 980 °C |
13300 psi @Temperature 1800 °F |
Hot-Rolled Plate, Solution-Annealed |
Special Metals INCOLOY® alloy 890 Ni-Cr-Fe Superalloy INCOLOY® alloy 890 (UNS N08890) is the latest addition to the INCOLOY alloy family of heat resistant alloys. Alloy 890 joins the existing INCOLOY products in offering high strength along with ex.. |
|||
Tensile Strength, Ultimate | 92.0 MPa @Temperature 80.0 °C |
13300 psi @Temperature 176 °F |
Absolute Drying; ASTM-D638 |
Toyobo GLAMIDE® T-402FR Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Tensile Strength, Ultimate | 92.0 MPa @Temperature 23.0 °C |
13300 psi @Temperature 73.4 °F |
Practical Use (Water Absorption 2.4%); ASTM-D638 |
Toyobo GLAMIDE® T-714E Transparent Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Tensile Strength, Ultimate | 92.0 MPa @Temperature 23.0 °C |
13300 psi @Temperature 73.4 °F |
ASTM D 638 |
Saint-Gobain Meldin® 2001 Bearing General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Series ca.. |