Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.351 - 0.526 kN/m | 2.00 - 3.00 pli | |
ITW Devcon 2 Ton® Epoxy Clear Epoxy, Clear, White Information provided by ITW Devcon |
|||
Peel Strength | 0.351 - 0.526 kN/m | 2.00 - 3.00 pli | |
ITW Devcon 5 minute® Epoxy Gel, Opaque Information provided by ITW Devcon |
|||
Peel Strength | 0.351 - 0.526 kN/m | 2.00 - 3.00 pli | |
ITW Devcon 5 minute® Epoxy, Light Amber Information provided by ITW Devcon |
|||
Peel Strength | 0.351 - 0.526 kN/m | 2.00 - 3.00 pli | |
ITW Devcon One minuteâ„¢ Epoxy Gel, Amber Information provided by ITW Devcon |