| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Viscosity | 8000 cP | 8000 cP | Mixed Viscosity |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Elongation at Break | 1.0 % | 1.0 % | |
| Adhesive Bond Strength | 15.5 MPa | 2250 psi | lap shear (on grit blasted steel, bond line thickness of 0.010"); ASTM D1002 |
| Tensile Impact Strength | 13.6 kJ/m² | 6.50 ft-lb/in² | |
| Peel Strength | 0.351 - 0.526 kN/m | 2.00 - 3.00 pli |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 93.3 °C | 200 °F | dry |
| Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | dry |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Transmission, Visible | 90 % | 90 % | clear; thickness not quantified |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time | 8.00 - 12.0 min | 0.133 - 0.200 hour | Working time |
| 30.0 - 35.0 min | 0.500 - 0.583 hour | Fixture time | |
| 120 min | 2.00 hour | Functional cure |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Mix ratio (Resin:Hardener) | 1:1 |